MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Lehvoss LUVOCOM® 1200-7116-1 ABS with carbon fiber
Categories: Polymer; Thermoplastic; ABS Polymer

Material Notes: Properties/attributes include: Reduced moment of inertia compared with metal parts. Electrically conductive, suitable for continuous discharging of statically-generated electricity. Strong, stiff parts.

Office communication.

Processing: During processing, the moisture content should not exceed 0.1%. Moisture may lead to smearing and in extreme cases to foaming. Usually the material can be processed over a broad temperature range and can thus be adapted to a wide variety of processing conditions. Temperatures >270°C may lead to thermal damage. The processing notes provided merely represent a recommendation for general use. Due to the large variety of machines, geometries and volumes of parts, etc., it may be necessary to employ different settings according to the specific application.

Information provided by Lehmann & Voss & Co.KG

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.09 g/cc1.09 g/ccISO 1183
Moisture Absorption <= 0.300 %
@Temperature 23.0 °C,
Time 86400 sec
<= 0.300 %
@Temperature 73.4 °F,
Time 24.0 hour
Linear Mold Shrinkage 0.0020 - 0.0040 cm/cm0.0020 - 0.0040 in/inDIN 16901
Melt Flow 14 g/10 min
@Load 10.0 kg,
Temperature 220 °C
14 g/10 min
@Load 22.0 lb,
Temperature 428 °F
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength 90.0 MPa13100 psiISO 527-2
Elongation at Break 1.5 %1.5 %ISO 527-2
Modulus of Elasticity 7.00 GPa1020 ksiISO 527-2
Flexural Strength 130 MPa18900 psiISO 178
Flexural Modulus 6.00 GPa870 ksiISO 178
Flexural Strain at Break 1.9 %1.9 %Flexural Elongation @ Fmax; ISO 178
Charpy Impact Unnotched 1.80 J/cm²
@Temperature 23.0 °C
8.57 ft-lb/in²
@Temperature 73.4 °F
ISO 179 1eU
Charpy Impact, Notched 0.600 J/cm²
@Temperature 23.0 °C
2.86 ft-lb/in²
@Temperature 73.4 °F
ISO 179 1eA
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity <= 1000 ohm-cm<= 1000 ohm-cmIEC 60167
Surface Resistance <= 10000 ohm<= 10000 ohmIEC 60093
 
Thermal PropertiesMetricEnglishComments
CTE, linear 40.0 µm/m-°C22.2 µin/in-°FDIN 53752
Thermal Conductivity 0.230 W/m-K1.60 BTU-in/hr-ft²-°FDIN 52612
Maximum Service Temperature, Air 60.0 °C140 °FContinuous; UL 746B
 80.0 °C176 °FShort Term
Deflection Temperature at 1.8 MPa (264 psi) 96.0 °C205 °FISO 75-2/A
Vicat Softening Point 100 °C212 °FVST A; DIN ISO 306
 
Processing PropertiesMetricEnglishComments
Nozzle Temperature 220 - 250 °C428 - 482 °F
Zone 1 220 - 250 °C428 - 482 °F
Zone 2 220 - 250 °C428 - 482 °F
Zone 3 230 - 260 °C446 - 500 °F
Melt Temperature 230 - 260 °C446 - 500 °F
Mold Temperature 40.0 - 80.0 °C104 - 176 °F
Drying Temperature 70.0 - 95.0 °C
@Time 7200 - 14400 sec
158 - 203 °F
@Time 2.00 - 4.00 hour
Dehumidifying dryer
Moisture Content <= 0.10 %<= 0.10 %
 
Descriptive Properties
Colorblack

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
RTP Company RTP 100 MG GB 15  Polypropylene (PP) Milled Glass - Glass Bead 15%
Lehvoss LUVOCOM® 1114-0717 PAEK with carbon fiber and PTFE

PLUU8865 / 193824

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.