MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

INEOS Styrolution Luran® HH-120 Alpha-Methylstyrene Acrylonitrile
Categories: Polymer; Thermoplastic; SAN Polymer

Material Notes: Luran HH-120 is a grade of AMSAN with high heat resistance and improved mechanical strength. It is suitable for injection molding and extrusion applications and can be used as a modifier for high heat ABS and PVC.
  • Outstanding heat resistance
  • Very good mechanical strength
  • Good surface appearance
  • Excellent dimensional stability
  • New SPF 50 UV stabilization available

Information provided by Styrolution

Key Words: AMSAN
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.08 g/cc0.0390 lb/in³ISO 1183
Moisture Absorption at Equilibrium 0.30 %
@Temperature 23.0 °C
0.30 %
@Temperature 73.4 °F
50% RH; ISO 62
Linear Mold Shrinkage 0.0030 - 0.0070 cm/cm0.0030 - 0.0070 in/inISO 294-4
Melt Flow 7.0 g/10 min
@Load 10.0 kg,
Temperature 220 °C
7.0 g/10 min
@Load 22.0 lb,
Temperature 428 °F
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell M 8484
Ball Indentation Hardness 175 MPa25400 psiISO 2039-1
Tensile Strength, Yield 79.0 MPa11500 psiISO 527
Elongation at Yield 3.0 %3.0 %ISO 527
Tensile Modulus 3.90 GPa566 ksiISO 527
Flexural Strength 135 MPa19600 psiISO 178
Izod Impact, Notched (ISO)  2.00 kJ/m²
@Temperature 23.0 °C
0.952 ft-lb/in²
@Temperature 73.4 °F
ISO 180/A
 2.00 kJ/m²
@Temperature -30.0 °C
0.952 ft-lb/in²
@Temperature -22.0 °F
ISO 180/A
Charpy Impact Unnotched  2.00 J/cm²
@Temperature 23.0 °C
9.52 ft-lb/in²
@Temperature 73.4 °F
ISO 179
 2.10 J/cm²
@Temperature -30.0 °C
9.99 ft-lb/in²
@Temperature -22.0 °F
ISO 179
Charpy Impact, Notched 0.200 J/cm²0.952 ft-lb/in²ISO 179
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity >= 1.00e+16 ohm-cm>= 1.00e+16 ohm-cmIEC 60093
Surface Resistance >= 1.00e+15 ohm>= 1.00e+15 ohmIEC 60093
Dielectric Constant 3.0
@Frequency 100 Hz
3.0
@Frequency 100 Hz
IEC 60250
Dissipation Factor  0.0050
@Frequency 100 Hz
0.0050
@Frequency 100 Hz
IEC 60250
 0.0070
@Frequency 1e+6 Hz
0.0070
@Frequency 1e+6 Hz
IEC 60250
 
Thermal PropertiesMetricEnglishComments
CTE, linear 70.0 µm/m-°C38.9 µin/in-°FISO 11359
Thermal Conductivity 0.170 W/m-K1.18 BTU-in/hr-ft²-°FDIN 52612-1
Deflection Temperature at 0.46 MPa (66 psi) 110 °C230 °FISO 75
Deflection Temperature at 1.8 MPa (264 psi) 104 °C219 °FISO 75
Vicat Softening Point 120 °C
@Load 5.10 kg
248 °F
@Load 11.2 lb
50°C/h; ISO 306
 
Optical PropertiesMetricEnglishComments
Refractive Index 1.567
@Wavelength 589.3 nm
1.567
@Wavelength 589.3 nm
Sodium D Line; ASTM D 542
Transmission, Visible >= 89 %
@Wavelength 550 nm
>= 89 %
@Wavelength 550 nm
ASTM D 1003
 
Processing PropertiesMetricEnglishComments
Melt Temperature 220 - 270 °C428 - 518 °FISO 294
Mold Temperature 60.0 °C140 °FISO 294
Injection Velocity 200 mm/sec7.87 in/secISO 294
Drying Temperature 80.0 °C
@Time 7200 - 14400 sec
176 °F
@Time 2.00 - 4.00 hour

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
INEOS Styrolution Luran® 358N SAN
Chi Mei Kibisan® PN-127 SAN
Chi Mei Kibisan® PN-117 SAN
INEOS Styrolution Luran® 348Q Transparent SAN
INEOS Styrolution Luran® 378P Crystal Clear Transparent SAN

PBASF8025 / 159707

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.