MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Armco 20-45-5 Iron-Nickel Alloy
Categories: Metal; Superalloy; Iron Base

Material Notes: Heat exchanger and condenser tubing, stress corrosion resistant

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesMetricEnglishComments
Rupture Strength  40.0 MPa
@Temperature 816 °C,
Time 3.60e+6 sec
5800 psi
@Temperature 1500 °F,
Time 1000 hour
 60.7 MPa
@Temperature 816 °C,
Time 360000 sec
8800 psi
@Temperature 1500 °F,
Time 100 hour
 75.8 MPa
@Temperature 732 °C,
Time 3.60e+6 sec
11000 psi
@Temperature 1350 °F,
Time 1000 hour
 110 MPa
@Temperature 732 °C,
Time 360000 sec
16000 psi
@Temperature 1350 °F,
Time 100 hour
 159 MPa
@Temperature 649 °C,
Time 3.60e+6 sec
23000 psi
@Temperature 1200 °F,
Time 1000 hour
 221 MPa
@Temperature 649 °C,
Time 360000 sec
32000 psi
@Temperature 1200 °F,
Time 100 hour
 
Component Elements PropertiesMetricEnglishComments
Carbon, C 0.050 %0.050 %
Chromium, Cr 20 %20 %
Iron, Fe 30.37 %30.37 %Balance
Manganese, Mn 4.0 %4.0 %
Nickel, Ni 45 %45 %
Niobium, Nb (Columbium, Cb) 0.15 %0.15 %
Silicon, Si 0.40 %0.40 %
Vanadium, V 0.030 %0.030 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Iron, Fe
AISI 1005 Steel
AISI 4340 Steel, normalized, 25 mm round
AK Steel ASTM A 1011, Grade 55 Hot Rolled Carbon Steel, Structural Steel (SS)
Aluminum 6061-T6; 6061-T651

NZ97049 / 191448

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.