MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Celanese Zytel® ST811HS NC010 PA6-HI
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6); Nylon 6, Impact Grade

Material Notes: Super Toughened, Heat Stabilized, Polyamide 6

Former DuPont product acquired by Celanese in 2022.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.04 g/cc0.0376 lb/in³DAM; ISO 1183
Melt Density 0.880 g/cc
@Temperature 270 °C
0.0318 lb/in³
@Temperature 518 °F
Water Absorption 6.8 %
@Thickness 2.00 mm
6.8 %
@Thickness 0.0787 in
DAM; Sim. to ISO 62
Moisture Absorption 2.30 %
@Thickness 2.00 mm
2.30 %
@Thickness 0.0787 in
DAM; Sim. to ISO 62
Linear Mold Shrinkage, Flow 0.0090 cm/cm0.0090 in/inDAM; ISO 294-4, 2577
Linear Mold Shrinkage, Transverse 0.014 cm/cm0.014 in/inDAM; ISO 294-4, 2577
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell M 6060DAM; ISO 2039-2
Tensile Strength, Yield 31.0 MPa4500 psiDAM; ISO 527-1/-2
Elongation at Break 4.0 %4.0 %parallel; DAM; ISO 527-3
 >= 50 %>= 50 %Nominal; DAM; ISO 527-1/-2
Elongation at Yield 29 %29 %DAM; ISO 527-1/-2
Tensile Modulus 0.400 GPa58.0 ksi50% RH; ISO 527-1/-2
 0.900 GPa131 ksiDAM; ISO 527-1/-2
Flexural Modulus 0.360 GPa52.2 ksi50% RH; ISO 178
 0.850 GPa123 ksiDAM; ISO 178
Poissons Ratio 0.450.45DAM
 0.470.4750% RH
Charpy Impact Unnotched  NB
@Temperature -30.0 °C
NB
@Temperature -22.0 °F
50% RH; ISO 179/1eU
 NB
@Temperature -30.0 °C
NB
@Temperature -22.0 °F
DAM; ISO 179/1eU
 NB
@Temperature 23.0 °C
NB
@Temperature 73.4 °F
50% RH; ISO 179/1eU
 NB
@Temperature 23.0 °C
NB
@Temperature 73.4 °F
DAM; ISO 179/1eU
Charpy Impact, Notched  1.30 J/cm²
@Temperature -30.0 °C
6.19 ft-lb/in²
@Temperature -22.0 °F
50% RH; ISO 179/1eA
 1.40 J/cm²
@Temperature -30.0 °C
6.66 ft-lb/in²
@Temperature -22.0 °F
DAM; ISO 179/1eA
 7.10 J/cm²
@Temperature 23.0 °C
33.8 ft-lb/in²
@Temperature 73.4 °F
DAM; ISO 179/1eA
 12.9 J/cm²
@Temperature 23.0 °C
61.4 ft-lb/in²
@Temperature 73.4 °F
50% RH; ISO 179/1eA
Puncture Energy  16.0 J
@Temperature 23.0 °C
11.8 ft-lb
@Temperature 73.4 °F
DAM; ISO 6603-2
 25.0 J
@Temperature -30.0 °C
18.4 ft-lb
@Temperature -22.0 °F
DAM; ISO 6603-2
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+13 ohm-cm1.00e+13 ohm-cm50% RH; IEC 62631-3-1
 1.00e+15 ohm-cm1.00e+15 ohm-cmDAM; IEC 62631-3-1
Surface Resistance 1.00e+15 ohm1.00e+15 ohm50% RH; IEC 62631-3-2
Dielectric Strength 31.0 kV/mm787 kV/inDAM; IEC 60243-1
Dissipation Factor  0.0080
@Frequency 100 Hz
0.0080
@Frequency 100 Hz
DAM; IEC 62631-2-1
 0.014
@Frequency 1e+6 Hz
0.014
@Frequency 1e+6 Hz
DAM; IEC 62631-2-1
 0.055
@Frequency 100 Hz
0.055
@Frequency 100 Hz
50% RH; IEC 62631-2-1
 0.18
@Frequency 1e+6 Hz
0.18
@Frequency 1e+6 Hz
50% RH; IEC 62631-2-1
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 200 µm/m-°C111 µin/in-°FDAM; ISO 11359-1/-2
CTE, linear, Transverse to Flow 180 µm/m-°C100 µin/in-°FDAM; ISO 11359-1/-2
Specific Heat Capacity 2.60 J/g-°C
@Temperature 270 °C
0.621 BTU/lb-°F
@Temperature 518 °F
Melt
Thermal Conductivity 0.150 W/m-K
@Temperature 270 °C
1.04 BTU-in/hr-ft²-°F
@Temperature 518 °F
Melt
Melting Point 218 °C424 °F10°C/min; DAM; ISO 11357-1/-3
Deflection Temperature at 1.8 MPa (264 psi) 47.0 °C117 °FDAM; ISO 75-1/-2
Vicat Softening Point 95.0 °C203 °F50°C/h, 50N; DAM; ISO 306
Glass Transition Temp, Tg 0.000 °C32.0 °F10°C/min; 50% RH; ISO 11357-1/-2
 50.0 °C122 °F10°C/min; DAM; ISO 11357-1/-2
Flammability, UL94  HB
@Thickness 0.750 mm
HB
@Thickness 0.0295 in
DAM; IEC 60695-11-10
 HB
@Thickness 1.50 mm
HB
@Thickness 0.0591 in
DAM; IEC 60695-11-10
Flame Spread <= 80.0 mm/min
@Thickness 1.00 mm
<= 3.15 in/min
@Thickness 0.0394 in
ISO 3795 (FMVSS 302)
 
Processing PropertiesMetricEnglishComments
Melt Temperature 240 °C464 °FOptimum, Extrusion
 235 - 250 °C455 - 482 °FRange, Extrusion
 260 - 280 °C500 - 536 °FRange, Injection
 270 °C518 °FOptimum, Injection
Mold Temperature 70.0 °C158 °FOptimum, Injection
 50.0 - 90.0 °C122 - 194 °FInjection
Ejection Temperature 190 °C374 °FInjection
Drying Temperature 60.0 °C140 °FInjection
 60.0 °C140 °FExtrusion
Dry Time 2.00 - 4.00 hour2.00 - 4.00 hourInjection, Dehumidified Dryer
 4.00 - 6.00 hour4.00 - 6.00 hourExtrusion, Dehumidified Dryer
Moisture Content <= 0.060 %<= 0.060 %Extrusion
 <= 0.20 %<= 0.20 %Injection
Hold Pressure 50.0 - 100 MPa7250 - 14500 psiRange, Injection
 
Descriptive Properties
AdditivesRelease agent
Drying RecommendedyesInjection
FMVSS ClassBISO 3795 (FMVSS 302)
ISO designationISO 16396-PA6-I,,M1G1HNR,S14-010
Max. screw tangential speed (m/s)0.3Injection
Part Marking Code>PA6-HI<ISO 11469
PolymerPA6-I
Processing Hold Pressure Time (s/mm)4Injection
Regional AvailabilityAsia Pacific
 Europe
 Near East/Africa
 North America
 South and Central America
Resin IdentificationPA6-HIISO 1043

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Celanese Zytel® ST7301 NC010 PA6-HI
Arkema Orgalloy® LE 60 LM XV NAT Polyamide 6 Alloy
Celanese Zytel® ST801 NC010A PA66-HI
Celanese Zytel® ST811HS BK038 PA6-HI
Celanese Zytel® ST7301 BK356 PA6-HI

PDSX5516 / 198156

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.