MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

INEOS Styrolution K-Resin® KR01 Styrene Butadiene Copolymer (SBC)
Categories: Polymer; Thermoplastic; Styrene-Butadiene; Styrene-Butadiene Copolymer, SBC

Material Notes: K-Resin® KR01 process very well in injection molding, providing good cycle times and design flexibility. Applications range from containers and packaging with living hinges to medical applications, toys, displays, overcaps and hangers. INEOS Styrolution has several grades of K-Resin® SBC tailored for your injection molded needs. Excellent Clarity, Good stiffness, good toughness, high surface gloss, warpage resistance. Applications: Molded boxes with integral hinges, medical devices, displays, toys.

Information provided by Styrolution.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.02 g/cc0.0368 lb/in³ISO 1183
Water Absorption at Saturation 0.070 %
@Temperature 23.0 °C
0.070 %
@Temperature 73.4 °F
ISO 62
Linear Mold Shrinkage 0.0030 - 0.010 cm/cm0.0030 - 0.010 in/inISO 294-4
Melt Flow 8.0 g/10 min
@Load 5.00 kg,
Temperature 200 °C
8.0 g/10 min
@Load 11.0 lb,
Temperature 392 °F
Volumetric; cm3/10 min; ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 7070ISO 868
Tensile Strength, Yield 33.0 MPa4790 psiISO 527
Elongation at Break 15 %15 %ISO 527
Elongation at Yield 2.8 %2.8 %ISO 527
Tensile Modulus 1.60 GPa232 ksiISO 527
Flexural Strength 43.0 MPa6240 psiISO 178
Flexural Modulus 1.50 GPa218 ksiISO 178
Charpy Impact Unnotched 2.70 J/cm²
@Temperature 23.0 °C
12.8 ft-lb/in²
@Temperature 73.4 °F
ISO 179/1eU
Charpy Impact, Notched 0.100 J/cm²
@Temperature 23.0 °C
0.476 ft-lb/in²
@Temperature 73.4 °F
ISO 179/1eA
 
Thermal PropertiesMetricEnglishComments
CTE, linear 60.0 - 90.0 µm/m-°C33.3 - 50.0 µin/in-°FISO 11359
Deflection Temperature at 0.46 MPa (66 psi) 78.0 °C172 °FISO 75
Deflection Temperature at 1.8 MPa (264 psi) 65.0 °C149 °Fannealed 4 hours at 80°C; ISO 75
Vicat Softening Point  65.0 °C
@Load 5.10 kg
149 °F
@Load 11.2 lb
VST/B/50. 50C/h; ISO 306
 91.0 °C
@Load 1.02 kg
196 °F
@Load 2.25 lb
VST/A/50. 50C/h; ISO 306
 
Optical PropertiesMetricEnglishComments
Refractive Index 1.571.57Sodium D Line; ISO 489
Haze 1.0 %1.0 %ASTM D 1003
Transmission, Visible 93 %
@Wavelength 550 nm
93 %
@Wavelength 550 nm
ASTM D1003

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
INEOS Styrolution K-Resin® KR03 Styrene Butadiene Copolymer (SBC)
A. Schulman Diamond SBS 1031 Clear Styrene Butadiene Copolymer
Kraton® D1118 K (SBS) Diblock Copolymer
Kraton® D1152 E (SBS) Liner Block Copolymer
Kraton® D1155 E (SBS) Liner Block Copolymer

PSTYR9870 / 216097

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.