MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Domo Technyl® A218 Heat Stabilized Nylon 66
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66); Nylon 66, Heat Stabilized

Material Notes: Information provided by Rhodia; Rhodia has been acquired by Solvay.

DOMO Chemicals has acquired Solvay’s Performance Polyamides Business in Europe.

Key Words: Polyamide 66; PA66
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.14 g/cc0.0412 lb/in³ASTM D792
Water Absorption 1.3 %1.3 %24 Hr.; ASTM D570
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 120120ASTM D785
Tensile Strength, Yield 90.3 MPa13100 psiASTM D638
Elongation at Break 40 %40 %ASTM D638
Tensile Modulus 3.00 GPa435 ksiASTM D638
Flexural Strength 120 MPa17400 psiASTM D790
Flexural Modulus 2.90 GPa421 ksiASTM D790
Izod Impact, Notched 0.502 J/cm0.940 ft-lb/inASTM D256
 
Thermal PropertiesMetricEnglishComments
Melting Point 255 °C491 °F
Deflection Temperature at 0.46 MPa (66 psi) 226 °C438 °FASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 82.2 °C180 °FASTM D648
Flammability, UL94 V-2
@Thickness 1.60 mm
V-2
@Thickness 0.0630 in
 
Processing PropertiesMetricEnglishComments
Feed Temperature 250 - 270 °C482 - 518 °F
Middle Barrel Temperature 260 - 280 °C500 - 536 °FCompression Zone
Front Barrel Temperature 270 - 300 °C518 - 572 °F
Nozzle Temperature 280 - 290 °C536 - 554 °F
Melt Temperature 270 - 290 °C518 - 554 °F
Mold Temperature 60.0 - 80.0 °C140 - 176 °FSurface
Drying Temperature 80.0 °C176 °FDehumidifying Dryer
Dry Time 3 - 4 hour3 - 4 hour
Moisture Content <= 0.20 %<= 0.20 %
Back Pressure 0.345 - 0.689 MPa50.0 - 100 psi
Fill Speed 300 - 600 mm/sec11.8 - 23.6 in/secPeripheral Screw Speed
 
Descriptive Properties
Injection Speed (cm3/sec)50 - 150 cm3/sec

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Celanese Zytel® 103HSL NC010 PA66
Domo Technyl® A 218 V30 Nylon 66, 30% Glass Fiber, EH0
Domo Technyl® A238 Unfilled, Heat Stabilized, Impact Modified Nylon 66
Domo TECHNYL® A 216 PA66, DRY
Domo Technyl® A 205F Nylon 66, EH0

PRHO03h / 65933

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.