MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Aptek 2100-A7C/B Low modulus urethane staking compound
Categories: Polymer; Adhesive; Thermoset; Polyurethane, TS; Thermoset Polyurethane, Adhesive

Material Notes: APTEK 2100-A7C/B is a thixotropic, two component, electrically insulating, low modulus urethane system designed for the staking of electrical/electronic components to printed circuit boards. Although APTEK 2100-A7C/B is capable of achieving full cure at room temperature, a short term exposure to moderate heat will greatly reduce processing time and optimize cured properties.

100% solids, solvent free system that will not form voids during cure or service life; Low Tg for excellent low-temperature cycling and performance; Very good substrate adhesion, superior to silicones; Exceeds NASA outgassing requirements for high vacuum environments

APTEK 2100-A7C is a translucent, filled polyol resin. APTEK 2100-B is a yellow/orange, organic isocyanate.

Information provided by Aptek Laboratories, Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.990 g/cc0.0358 lb/in³A Component; ASTM D1475
 1.21 g/cc0.0437 lb/in³B Component; ASTM D1475
Viscosity 35 cP35 cPB Component; ASTM D1824
Outgassing - Total Mass Loss 0.38 %0.38 %Cured property; at 10E-6 torr; ASTM E-595
Collected Volatile Condensable Material 0.030 %0.030 %Cured property; at 10E-6 torr; ASTM E595
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 5555Cured property; ASTM D2240
Tensile Strength, Ultimate 2.76 MPa400 psiCured property; ASTM D412
Elongation at Break 265 %265 %Cured property; ASTM D412
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 5.30e+15 ohm-cm5.30e+15 ohm-cmCured property; ASTM D257
Dielectric Constant 3.5
@Frequency 1000 Hz
3.5
@Frequency 1000 Hz
Cured property; ASTM D150
Dielectric Strength >= 14.2 kV/mm>= 360 kV/inCured property; 0.1 inch; ASTM D149
Dissipation Factor 0.030
@Frequency 1000 Hz
0.030
@Frequency 1000 Hz
Cured property; ASTM D150
 
Thermal PropertiesMetricEnglishComments
CTE, linear  79.0 µm/m-°C
@Temperature 20.0 °C
43.9 µin/in-°F
@Temperature 68.0 °F
Cured property; alpha 1; JMTP P200
 185 µm/m-°C
@Temperature 20.0 °C
103 µin/in-°F
@Temperature 68.0 °F
Cured property; alpha 2; JMTP P200
Glass Transition Temp, Tg -70.0 °C-94.0 °FCured property; JMTP 200
Flash Point >= 150 °C>= 302 °FA Component; ASTM D92
 >= 150 °C>= 302 °FB Component; ASTM D92
 
Processing PropertiesMetricEnglishComments
Processing Temperature 80.0 °C176 °FCure 5 hrs + 2 hrs at RT
 100 °C212 °FCure 3 hrs + 2 hrs at RT

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
AorTech Biomaterials ECSil™ 70A Biomedical Carbonate Silicone Pellets
Aptek 2120 PMF Low modulus urethane staking compound
Aptek 2205 A/B Low modulus urethane stacking compound
Aptek UVISTAKE 7205LM-PMF UV Curing, Low Outgassing, Urethane staking compound
Alliance Polymers Zythane™ 6080A Thermoplastic Polyurethane Elastomer

PAPTEK22 / 24184

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.