Product description: Grivory HTV-45H1 black 9205 is a 45% glass fiber reinforced engineering thermoplastic material based on a semi-crystalline, partially aromatic copolyamide. Polymer designation acc. to ISO: PA 6T/6I Acc. to ASTM: PPA, polyphthalamide. Grivory HTV-45H1 black 9205 is an injection molding material. The main distinguishing feature of Grivory HT, when compared to other polyamides, is its good performance at high temperatures providing parts which are stiffer, stronger and have better heat distortion stability and chemical resistance. Grivory HT is suitable for production of technical parts in the application fields of:- Electro
- Electronics
- Automotive
- Mechanical engineering
- Domestic appliance
Information provided by EMS Grivory |