MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

China-Yixing Longly Refractories Microcrystal Wear-Resistant Alumina Grinding Media (Balls) and Lining Bricks
Categories: Ceramic; Oxide; Aluminum Oxide

Material Notes: LONGLY adopts isostatic pressing and dry pressing in the forming process and provides a variety of products with different dimension and specification. These products are extremely hard (9 on Moh's scale, only inferior to Diamond), fully dense, corrosion resistance, low wear loss, high grinding efficiency, no contamination on the material being ground. They are resistant to most acids and alkalis, except HF.

Applications: Applicable to the lining and grinding media of milling equipment, such as ball mill, polishing machine and luster polish machine, which are used to grind all kinds of ceramic materials, refractories, cement, alpha-alumina powder, Kaolin, fused corundum material, mechanical catalyst, fluorescence material, ceramic glaze, pigment, paint and coating.

Information Provided by China Yixing Longly Refractories Co. Ltd

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 3.55 - 3.65 g/cc0.128 - 0.132 lb/in³
Water Absorption <= 0.020 %<= 0.020 %
 
Mechanical PropertiesMetricEnglishComments
Hardness, Mohs 9.09.0
Compressive Strength 1500 - 2200 MPa218000 - 319000 psiCrushing Strength
Fracture Toughness 5.60 - 6.80 MPa-m½5.10 - 6.19 ksi-in½
 
Component Elements PropertiesMetricEnglishComments
Al2O3 90 - 95 %90 - 95 %
Fe2O3 0.20 - 0.30 %0.20 - 0.30 %
 
Descriptive Properties
Wear Loss (%)0.10-0.20

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Chosun Refractories SSB-3 Bricks, Reaction Bonded SiC
Skamol Group SUPER 1100 ET Calcium Silicate Insulating Slab
Chosun Refractories AB10L Alumina Magnesia Carbon Bricks for Ladle Wall And Bottom
Chosun Refractories AB10H Alumina Magnesia Carbon Bricks for Ladle Wall And Bottom
Reade Advanced Materials Diatomaceous Earth (DE) (SiO2·nH2O)

CYXLR022 / 99324

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.