MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Arkema LOTADER® 4403 Terpolymer Ethylene - Acrylic Ester - Maleic Anhydride
Categories: Polymer; Thermoplastic; EMAAA Terpolymer

Material Notes: LOTADER 4403 is a random terpolymer of Ethylene, Acrylic Ester and Maleic Anhydride, polymerized by high pressure autoclave process.

LOTADER 4403 is a versatile adhesive for extrusion lamination, designed as a ready for use resin to be used pure. LOTADER 4403 gives excellent adhesion to aluminium foil in the extrusion lamination process. It also bonds to PE films, paper, board, metallized plastics and corona treated plastics like OPP, CPP and OPA. Typical uses are:

  • Adhesive for extrusion lamination of polar and non polar films and foils, particularly for laminates involving aluminium.
  • Adhesive for coextrusion coating of LDPE / Tie / PA / tie onto paper or films.

Information provided by Arkema Group

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.940 g/cc
@Temperature 23.0 °C
0.0340 lb/in³
@Temperature 73.4 °F
ISO 1183
Methyl Acrylate Content 20 %20 %IRTF (internal)
Melt Index of Compound 9.0 g/10 min
@Load 2.16 kg,
Temperature 190 °C
9.0 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 2525ASTM D2240
Tensile Strength at Break 9.60 MPa1390 psiASTM D638
Elongation at Break 750 %750 %ASTM D638
Flexural Modulus 0.0200 GPa2.90 ksiASTM D638
 
Thermal PropertiesMetricEnglishComments
Melting Point 77.0 °C171 °FDSC
Vicat Softening Point 45.0 °C
@Load 0.999 kg
113 °F
@Load 2.20 lb
ASTM D1525
 
Processing PropertiesMetricEnglishComments
Processing Temperature 270 - 330 °C518 - 626 °F
 
Descriptive Properties
Maleic Anhydride Content (%)0.3IRTF (internal)

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Arkema LOTADER® 8200 Terpolymer Ethylene - Acrylic Ester - Maleic Anhydride
Arkema LOTADER® 3430 Terpolymer Ethylene - Acrylic Ester - Maleic Anhydride
Arkema LOTADER® 5500 Terpolymer Ethylene - Acrylic Ester - Maleic Anhydride
Arkema LOTADER® 3410 Terpolymer Ethylene - Acrylic Ester - Maleic Anhydride
Arkema LOTADER® 4503 Terpolymer Ethylene - Acrylic Ester - Maleic Anhydride

PARKG184 / 80084

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.