MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Overview of materials for Chlorinated PVC (CPVC)
Categories: Polymer; Thermoplastic; Vinyl (PVC); Chlorinated PVC (CPVC)

Material Notes: This property data is a summary of similar materials in the MatWeb database for the category "Chlorinated PVC (CPVC)". Each property range of values reported is minimum and maximum values of appropriate MatWeb entries. The comments report the average value, and number of data points used to calculate the average. The values are not necessarily typical of any specific grade, especially less common values and those that can be most affected by additives or processing methods.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.45 - 1.65 g/cc0.0524 - 0.0596 lb/in³Average value: 1.52 g/cc Grade Count:23
Viscosity 1.30 - 1.60 cP1.30 - 1.60 cPAverage value: 1.41 cP Grade Count:4
Viscosity Number 72.0 - 94.0 cm³/g0.720 - 0.940 dl/gAverage value: 79.3 cm³/g Grade Count:3
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 111 - 119111 - 119Average value: 116 Grade Count:10
Hardness, Shore D 80.0 - 90.080.0 - 90.0Average value: 83.7 Grade Count:7
Tensile Strength, Ultimate 9.00 - 80.0 MPa1310 - 11600 psiAverage value: 49.0 MPa Grade Count:13
Tensile Strength, Yield 48.4 - 58.0 MPa7020 - 8410 psiAverage value: 53.0 MPa Grade Count:16
Elongation at Break 15.0 - 650 %15.0 - 650 %Average value: 119 % Grade Count:6
Elongation at Yield 2.30 - 7.00 %2.30 - 7.00 %Average value: 4.88 % Grade Count:5
Modulus of Elasticity 2.20 - 3.10 GPa319 - 450 ksiAverage value: 2.65 GPa Grade Count:23
Flexural Yield Strength 73.1 - 108 MPa10600 - 15700 psiAverage value: 92.5 MPa Grade Count:13
Flexural Modulus 2.69 - 3.50 GPa390 - 508 ksiAverage value: 2.92 GPa Grade Count:12
Izod Impact, Notched 0.694 - 4.50 J/cm1.30 - 8.43 ft-lb/inAverage value: 1.57 J/cm Grade Count:13
Izod Impact, Notched (ISO) 10.0 - 12.0 kJ/m²4.76 - 5.71 ft-lb/in²Average value: 10.6 kJ/m² Grade Count:10
 2.31 - 2.31 kJ/m²
@Temperature 0.000 - 0.000 °C
1.10 - 1.10 ft-lb/in²
@Temperature 32.0 - 32.0 °F
Average value: 2.31 kJ/m² Grade Count:1
 2.31 - 2.31 kJ/m²
@Thickness 3.18 - 3.18 mm
1.10 - 1.10 ft-lb/in²
@Thickness 0.125 - 0.125 in
Average value: 2.31 kJ/m² Grade Count:1
Charpy Impact Unnotched 1000 J/cm² - NB4760 ft-lb/in² - NBGrade Count:5
Charpy Impact, Notched 1.00 - 2.70 J/cm²4.76 - 12.8 ft-lb/in²Average value: 1.43 J/cm² Grade Count:5
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 1.8 MPa (264 psi) 78.9 - 115 °C174 - 239 °FAverage value: 104 °C Grade Count:16
Vicat Softening Point 98.0 - 115 °C208 - 239 °FAverage value: 108 °C Grade Count:16
Decomposition Temperature 110 - 120 °C230 - 248 °FAverage value: 115 °C Grade Count:8
Flammability, UL94 V-0 - 5VAV-0 - 5VAGrade Count:9
Oxygen Index 56.0 - 75.0 %56.0 - 75.0 %Average value: 66.8 % Grade Count:7
 
Processing PropertiesMetricEnglishComments
Melt Temperature 191 - 210 °C376 - 410 °FAverage value: 203 °C Grade Count:10
 
Component Elements PropertiesMetricEnglishComments
Chlorine, Cl 32.0 - 69.0 %32.0 - 69.0 %Average value: 59.8 % Grade Count:5

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Overview of materials for Polyetheretherketone, Unreinforced
Multibase TPSiV® 3010-60A Thermoplastic Silicone Vulcanizate
Overview of materials for PVC, Rigid Grade
Overview of materials for PVC, Extruded
Geon® Performance Solutions CPVC LC500 Polyvinyl Chloride, Chlorinated (CPVC)

O5660 / 78525

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.