MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

EMS-Grivory Grilon® TSC-30/4 LF 15 black 9832 PA666-(CF+Z)45
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6/66

Material Notes: Product description: Grilon TSC-30/4 LF 15 is a heat stabilized, normal viscosity PA66 + PA6 injection molding grade with 30% carbon fibers and 15% of a combination of PTFE and silicone oil. Grilon TSC-30/4 LF 15 has the following important properties:
  • Electrical conductive
  • Very high stiffness
  • Excellent sliding friction characteristics
Grilon TSC-30/4 LF 15 is used typically for slide bearing applications such as shaft bearing rings, gears, and planetary gears.

Information provided by EMS Grivory.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.40 g/cc0.0506 lb/in³Dry; ISO 1183
Water Absorption 5.0 %5.0 %Sim. to ISO 62
Moisture Absorption 1.50 %1.50 %Sim. to ISO 62
Linear Mold Shrinkage, Flow 0.0010 cm/cm0.0010 in/inISO 294-4, 2577
Linear Mold Shrinkage, Transverse 0.0010 cm/cm0.0010 in/inISO 294-4, 2577
 
Mechanical PropertiesMetricEnglishComments
Ball Indentation Hardness 120 MPa17400 psiConditioned; ISO 2039-1
 210 MPa30500 psiDry; ISO 2039-1
Tensile Strength at Break 170 MPa24700 psiConditioned; ISO 527-1/-2
 230 MPa33400 psiDry; ISO 527-1/-2
Elongation at Break 2.5 %2.5 %Dry; ISO 527-1/-2
 4.5 %4.5 %Conditioned; ISO 527-1/-2
Tensile Modulus 16.0 GPa2320 ksiConditioned; ISO 527-1/-2
 23.0 GPa3340 ksiDry; ISO 527-1/-2
Charpy Impact Unnotched  4.50 J/cm²
@Temperature -30.0 °C
21.4 ft-lb/in²
@Temperature -22.0 °F
Dry; ISO 179/1eU
 4.50 J/cm²
@Temperature 23.0 °C
21.4 ft-lb/in²
@Temperature 73.4 °F
Dry; ISO 179/1eU
 4.50 J/cm²
@Temperature -30.0 °C
21.4 ft-lb/in²
@Temperature -22.0 °F
Conditioned; ISO 179/1eU
 6.00 J/cm²
@Temperature 23.0 °C
28.6 ft-lb/in²
@Temperature 73.4 °F
Conditioned; ISO 179/1eU
Charpy Impact, Notched  0.700 J/cm²
@Temperature -30.0 °C
3.33 ft-lb/in²
@Temperature -22.0 °F
Dry; ISO 179/1eA
 0.700 J/cm²
@Temperature -30.0 °C
3.33 ft-lb/in²
@Temperature -22.0 °F
Conditioned; ISO 179/1eA
 1.00 J/cm²
@Temperature 23.0 °C
4.76 ft-lb/in²
@Temperature 73.4 °F
Dry; ISO 179/1eA
 1.30 J/cm²
@Temperature 23.0 °C
6.19 ft-lb/in²
@Temperature 73.4 °F
Conditioned; ISO 179/1eA
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1000 ohm-cm1000 ohm-cmDry; IEC 60093
 1000 ohm-cm1000 ohm-cmConditioned; IEC 60093
Surface Resistance 1000 ohm1000 ohmIEC 60093
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 10.0 µm/m-°C5.56 µin/in-°FISO 11359-1/-2
CTE, linear, Transverse to Flow 80.0 µm/m-°C44.4 µin/in-°FISO 11359-1/-2
Melting Point 260 °C500 °F10°C/min; ISO 11357-1/-3
Maximum Service Temperature, Air 90.0 - 120 °C194 - 248 °FLong Term; ISO 2578
 200 °C392 °FShort Term; EMS
Deflection Temperature at 1.8 MPa (264 psi) 235 °C455 °FISO 75-1/-2
Deflection Temperature at 8.0 MPa 130 °C266 °FISO 75-1/-2
Flammability, UL94 HBHBIEC 60695-11-10
 
Descriptive Properties
AutomotiveAutomotive electr. and electronics, lighting
 Powertrain and Chassis
Electricals & ElectronicsElectrical appliances
 Electrical equipment
FormGranules
Industry & Consumer goodsMechanical Engineering
 Power transmission
 Sports & Leisure
 Tools & Accessories
ProcessingInjection Molding
Product AttributesImproved friction & wear properties
Special CharacteristicsAnti-static

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
EMS-Grivory Grilon® TSC-30/4 EC black 9832 PA666-CF30
Overview of materials for Nylon 66, 10% Carbon Fiber Filled
EMS-Grivory Grivory® HT2C-3X black 9833 PA6T/66-CF30
Overview of materials for Nylon 66, 30% Carbon Fiber Filled
Overview of materials for Nylon 66/6, 30% Glass Fiber Reinforced

PGRH255 / 156964

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.