MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Antimony, Sb
Categories: Metal; Nonferrous Metal; Pure Element

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 6.618 g/cc0.2391 lb/in³
 
Chemical PropertiesMetricEnglishComments
Atomic Mass 121.760121.7601995
Atomic Number 5151
Thermal Neutron Cross Section 5.7 barns/atom5.7 barns/atom
X-ray Absorption Edge 0.40663 Å0.40663 ÅK
 2.63296 Å2.63296 ÅLI
 2.82304 Å2.82304 ÅLII
 2.99637 Å2.99637 ÅLIII
Electrode Potential 0.10 V0.10 V
Electronegativity 2.052.05Pauling
Ionic Radius 0.620 Å0.620 ÅCrystal Ionic Radius for Valence +5
 0.760 Å0.760 ÅCrystal Ionic Radius for Valence +3
 2.45 Å2.45 ÅCrystal Ionic Radius for Valence -3
Electrochemical Equivalent 1.494 g/A/h1.494 g/A/h
 
Mechanical PropertiesMetricEnglishComments
Hardness, Brinell 30 - 5830 - 58
Hardness, Vickers 30 - 6030 - 60
Tensile Strength, Ultimate 11.4 MPa1650 psi
Modulus of Elasticity 77.759 GPa11278 ksi
Shear Modulus 19.0 GPa2760 ksi
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.0000410 ohm-cm0.0000410 ohm-cm
Magnetic Susceptibility -8.13e-7-8.13e-7cgs/g
Critical Superconducting Temperature 2.60 - 2.70 K2.60 - 2.70 K
 3.40 - 3.55 K
@Pressure 8500 - 15000 MPa
3.40 - 3.55 K
@Pressure 1.23e+6 - 2.18e+6 psi
Sb III
 
Thermal PropertiesMetricEnglishComments
Heat of Fusion 168.3 J/g72.40 BTU/lb
Heat of Vaporization 1604 J/g690.0 BTU/lb
CTE, linear 10.9 µm/m-°C
@Temperature 20.0 - 100 °C
6.06 µin/in-°F
@Temperature 68.0 - 212 °F
Specific Heat Capacity 0.206 J/g-°C0.0492 BTU/lb-°F
Thermal Conductivity 18.6 W/m-K129 BTU-in/hr-ft²-°F
Melting Point 630.74 °C1167.3 °F
Boiling Point 1587 °C2889 °F
 
Optical PropertiesMetricEnglishComments
Reflection Coefficient, Visible (0-1) 0.700.7058.9 micron wavelength
 
Component Elements PropertiesMetricEnglishComments
Antimony, Sb 100 %100 %
 
Descriptive Properties
CAS Number7440-36-0

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Silver, Ag
Bismuth, Bi
Gallium, Ga
Sodium, Na
Cesium, Cs

AMESb00 / 99

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.