MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Albis Plastics Tedur® L V 9107-1 PPS, 40% Glass Fiber  (discontinued **)
Categories: Polymer; Thermoplastic; Polyphenylene Sulfide (PPS); Polyphenylene Sulfide (PPS) with 40% Glass Fiber Filler

Material Notes: Low Flash, Improved Impact and Burst Strength. Incandescent wire resistance (2 mm) is 960°C per VDE 0471 T1.2.

Applications: Pump Housings, Hollow Articles Under Pressure

Processing: Injection Molding (Melt Temperature: 610-645°F, Mold Temperature: 285°F)

Tedur® is manufactured by Albis Plastics Corporation under license of the registered trademark owner (Bayer.) Data supplied by Albis Plastics Corporation.

Former ALBIS Plastics product lines have been spun off under the MOCOM brand. This specific grade was discontinued prior to the spin off.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.65 g/cc0.0596 lb/in³DIN 53 47
 
Mechanical PropertiesMetricEnglishComments
Flexural Yield Strength 250 MPa36300 psiDIN 53 452
Flexural Modulus 12.0 GPa1740 ksiDIN 53 457
Izod Impact, Notched 4.48 J/cm8.39 ft-lb/inApproximation; ISO 180/1U
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 1.8 MPa (264 psi) 260 °C500 °FASTM D648
Flammability, UL94 V-0V-0Albis Internal Test
 
Processing PropertiesMetricEnglishComments
Melt Temperature 321 - 341 °C610 - 646 °FInjection
Mold Temperature 141 °C286 °F

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Celanese FORTRON 1140L4 PPS, 40% Glass Reinforced
Overview of materials for Polyphenylene Sulfide (PPS) with 40% Glass Fiber Filler
Albis Plastics Tedur® L V 9300-1 PPS, 40% Glass Fiber/Glass Bead
Albis Plastics Tedur® L V 9400-1 PPS, 15% Carbon Fiber
Afton Plastics 440HP PFA Compression Molded Rod

PA1D37 / 21932

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.