MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Mitsui TPX® MX004 Methylpentene Copolymer
Categories: Polymer; Thermoplastic; Polymethylpentene (PMP)

Material Notes: TPX® is a 4-methylpentene-1 based polyolefin. TPX is used in a wide variety of applications, including: medical equipment, laboratory ware, small appliances, ovenware, baking cartons, release paper, wire and cable coating, and a number of industrial uses. TPX is manufactured and marketed solely by Mitsui Chemicals, Inc.

Applications:

  • Injection Molded Items:
    • Blood test cells
    • Medical instruments
    • Laboratory ware
    • Coffee maker parts
    • Cosmetic containers
  • Extrusion Molded Items:
    • Sight glass (pipes, sheets)
    • Baking cartons (food containers)
    • Release paper
    • Wire and cable coating
    • Films

Molding Method:

  • Injection
  • Extrusion

Information provided by Mitsui.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.834 g/cc0.0301 lb/in³ASTM D1505
Water Absorption 0.010 %0.010 %24 hours; ASTM D570
Linear Mold Shrinkage 0.019 cm/cm0.019 in/inMPC method, MD
Linear Mold Shrinkage, Transverse 0.017 cm/cm0.017 in/inMPC method
Melt Flow 26 g/10 min
@Load 5.00 kg,
Temperature 260 °C
26 g/10 min
@Load 11.0 lb,
Temperature 500 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 6060ASTM D785
Tensile Strength at Break 17.2 MPa2490 psi5mm/min; ASTM D638
Tensile Strength, Yield 19.6 MPa2840 psi5mm/min; ASTM D638
Elongation at Break 85 %85 %MPC method, 5mm/min
Modulus of Elasticity 0.740 GPa107 ksiTangent; ASTM D790
Flexural Strength 24.5 MPa3550 psi2mm/min; ASTM D790
Flexural Stiffness 621 MPa90000 psiOlsen Stiffness; ASTM D747
Izod Impact, Unnotched (ISO) 48.3 kJ/m²
@Thickness 2.00 mm,
Temperature 20.0 °C
23.0 ft-lb/in²
@Thickness 0.0787 in,
Temperature 68.0 °F
ASTM D256
Charpy Impact, Notched 0.420 J/cm²
@Thickness 2.00 mm,
Temperature 20.0 °C
2.00 ft-lb/in²
@Thickness 0.0787 in,
Temperature 68.0 °F
ASTM D256
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity >= 1.00e+16 ohm-cm>= 1.00e+16 ohm-cmASTM D257
Dielectric Constant 2.12
@Frequency 100 - 1.00e+6 Hz
2.12
@Frequency 100 - 1.00e+6 Hz
ASTM D150
Dielectric Strength 65.0 kV/mm1650 kV/inASTM D149
 
Thermal PropertiesMetricEnglishComments
CTE, linear 117 µm/m-°C
@Temperature 20.0 °C
65.0 µin/in-°F
@Temperature 68.0 °F
ASTM D696
Specific Heat Capacity 1.97 J/g-°C0.471 BTU/lb-°FASTM C351
Thermal Conductivity 0.167 W/m-K1.16 BTU-in/hr-ft²-°FBS 874A
Melting Point 240 °C464 °FMPC Method
Deflection Temperature at 0.46 MPa (66 psi) 85.0 °C185 °FASTM D648
Vicat Softening Point 160 °C320 °FASTM D1525
 
Optical PropertiesMetricEnglishComments
Refractive Index 1.4631.463n20 D; ASTM D542
Haze 1.0 %1.0 %ASTM D1746
Transmission, Visible 90 %90 %Mfr. indicates clear but does not quantify
 
Descriptive Properties
AppearanceColorless transparent
Rate of Burning2.54 cm/minASTM D635

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
EMS-Grivory Grilamid® TR 30 nat PA*
Mitsui TPX® MX002 Methylpentene Copolymer
EMS-Grivory Grilamid® TR 90 UV PAMACM12
Westlake Plastics TPX® Polymethylpentene
Mitsui TPX® RT18 Methylpentene Copolymer, Transparent Grade

PMIT050 / 53231

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.