MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Mocom (ALBIS) ALTECH® PA6 A 2030/109 GF30 BK0004-00LS Nylon 6, 30% Glass Fiber Reinforced, Dry
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6); Nylon 6, 30% Glass Fiber Filled

Material Notes: Base Polymer: Polyamide 6

Filler/Additive System: 30% glass fibers

Special Features: Heat ageing stabilization, easy release (demolding), high flow, fast solidifying, laser etchable (light etching)

Typical Application: Housings, various

Information provided by Albis Plastics

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.36 g/cc0.0491 lb/in³ISO 1183
Maximum Moisture Content 0.150.15
Linear Mold Shrinkage, Flow 0.0010 - 0.0030 cm/cm
@Time 86400 sec
0.0010 - 0.0030 in/in
@Time 24.0 hour
ISO 294-4
Linear Mold Shrinkage, Transverse 0.0060 - 0.0080 cm/cm
@Time 86400 sec
0.0060 - 0.0080 in/in
@Time 24.0 hour
ISO 294-4
Storage Temperature <= 30.0 °C<= 86.0 °Fdry, protected from light
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 140 MPa20300 psiISO 527
Elongation at Break 2.5 %2.5 %ISO 527
Tensile Modulus 9.40 GPa1360 ksiISO 527
Flexural Strength 205 MPa29700 psiISO 178
Flexural Modulus 8.00 GPa1160 ksiISO 178
Charpy Impact Unnotched  5.50 J/cm²
@Temperature -40.0 °C
26.2 ft-lb/in²
@Temperature -40.0 °F
ISO 179/1eU
 6.50 J/cm²
@Temperature 23.0 °C
30.9 ft-lb/in²
@Temperature 73.4 °F
ISO 179/1eU
Charpy Impact, Notched  0.650 J/cm²
@Temperature -40.0 °C
3.09 ft-lb/in²
@Temperature -40.0 °F
ISO 179/1eA
 0.900 J/cm²
@Temperature 23.0 °C
4.28 ft-lb/in²
@Temperature 73.4 °F
ISO 179/1eA
 
Thermal PropertiesMetricEnglishComments
Melting Point 220 °C428 °FISO 11357
Deflection Temperature at 1.8 MPa (264 psi) 210 °C410 °FISO 75-1/-2
Vicat Softening Point 214 °C417 °FB50; ISO 306
Flammability, UL94 HB
@Thickness 0.750 mm
HB
@Thickness 0.0295 in
 
Processing PropertiesMetricEnglishComments
Melt Temperature 270 - 290 °C518 - 554 °FInjection molding
Mold Temperature 80.0 - 100 °C176 - 212 °FInjection molding
Drying Temperature <= 80.0 °C
@Time 7200 - 43200 sec
<= 176 °F
@Time 2.00 - 12.0 hour
in a dry air (desiccant) dryer
 
Descriptive Properties
Base PolymerPolyamide 6

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Mocom (ALBIS) ALTECH® PA66 B 2030/109 GF30 Nylon 66, 30% Glass Fiber Reinforced
Mocom (ALBIS) ALTECH® PA66 A 2030/109 GF30 Nylon 66, 30% Glass Fiber Reinforced
Mocom (ALBIS) ALTECH® PA66 A 2030/109 GF30 GY1176-12LS Nylon 66, 30% Glass Fiber Reinforced, Dry
Mocom (ALBIS) ALTECH® PA6 A 2030/319 GF30 IM Nylon 6, 30% Glass Fiber Reinforced

PALBIS8659 / 242718

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.