MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

G-10 Fiberglass Epoxy Laminate Sheet
Categories: Polymer; Thermoset; Epoxy; Filled/Reinforced Thermoset

Material Notes: This glass-epoxy laminate is specified for its extremely high strength and high dimensional stability over temperature. G-10 is used for terminal boards, high humidity applications, electrical and electronic test equipment and electric rotor insulation. G-10 is difficult to cut or machine and may require special equipment. G-10 is slightly stronger while G-11 is a better insulator and can withstand higher temperatures. FR-4 is a fire-retardant G-10 glass-epoxy laminate that is used primarily in the printed circuit board industry. G-10 and similar fiberglass reinforced thermosets are sometimes known as garolite.

Information provide by Boedeker Plastics.

Key Words: G10 Fiber Reinforced Composite
Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 1.80 g/cc0.0650 lb/in³ASTM D792
Water Absorption 0.10 %0.10 %24 hrs.; ASTM D570
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell M 110110ASTM D785
Tensile Strength at Break 262 MPa38000 psiCrosswise; ASTM D638
 310 MPa45000 psiLengthwise; ASTM D638
Flexural Strength 448 MPa65000 psiCrosswise; ASTM D790
 517 MPa75000 psiLengthwise; ASTM D790
Flexural Modulus 16.5 GPa2400 ksiCrosswise; ASTM D790
 18.6 GPa2700 ksiLengthwise; ASTM D790
Compressive Strength 448 MPa65000 psiASTM D695
Izod Impact, Notched 6.41 J/cm12.0 ft-lb/inCrosswise; ASTM D256
 7.47 J/cm14.0 ft-lb/inLengthwise; ASTM D256
 
Electrical PropertiesMetricEnglishComments
Dielectric Constant 5.0
@Frequency 1e+6 Hz
5.0
@Frequency 1e+6 Hz
ASTM D150
Dielectric Strength 31.5 kV/mm800 kV/inShort Time; 1/8 inch; ASTM D149
Dissipation Factor 0.019
@Frequency 1e+6 Hz
0.019
@Frequency 1e+6 Hz
ASTM D150
Arc Resistance 100 sec100 secASTM D495
 
Thermal PropertiesMetricEnglishComments
CTE, linear 9.90 µm/m-°C
@Temperature 20.0 °C
5.50 µin/in-°F
@Temperature 68.0 °F
Lengthwise; ASTM D696
CTE, linear, Transverse to Flow 11.9 µm/m-°C
@Temperature 20.0 °C
6.61 µin/in-°F
@Temperature 68.0 °F
Crosswise; ASTM D696
Thermal Conductivity 0.288 W/m-K2.00 BTU-in/hr-ft²-°FASTM C177
Maximum Service Temperature, Air 140 °C284 °F
Flammability, UL94 HBHB

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Elektro-Isola G-Etronax EP FR4 Epoxy, Glass Fabric Reinforcement, Light Yellow, Sheets
G-11 Fiberglass Epoxy Laminate Sheet
Polymer Resources PPX-FR4 Modified-PPO, V-1 Flame Retardant
Ensinger TECAPEI® 10% Glass Reinforced, made from Ultem® 2100 PEI
Overview of materials for Nylon 6, 30% Glass Fiber Filled

PGLAM04 / 41889

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.