MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

FKuR Kunststoff Biograde® C 7500 Biodegradable Plastic Compound  (discontinued **)
Categories: Polymer; Renewable/Recycled Polymer; Thermoplastic; Wood and Natural Products

Material Notes: BIOGRADE® are easy to process blends based on cellulose. BIOGRADE® is composed mainly of natural resources. Based on cellulose, a product of the paper industry BIOGRADE® has been especially designed for injection molding applications. BIOGRADE® is mainly composed of natural resource materials (European Soft Wood from sustainable forestry) and does not contain starch or starch derivatives.

Information Provided by FKuR Kunststoff GmbH

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Bulk Density 0.760 g/cc0.0275 lb/in³ISO 60
Density 1.31 g/cc0.0473 lb/in³ISO 1183
Melt Flow 17 - 21 g/10 min
@Load 5.00 kg,
Temperature 230 °C
17 - 21 g/10 min
@Load 11.0 lb,
Temperature 446 °F
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 8080
Tensile Strength at Break 65.0 MPa9430 psiISO 527
Tensile Strength 66.0 MPa9570 psiISO 527
Elongation at Break 12.5 %12.5 %ISO 527
Elongation at Yield 12.5 %12.5 %ISO 527
Tensile Modulus 3.00 GPa435 ksiISO 527
Flexural Strength 70.0 MPa10200 psiat 3.5% strain;; ISO 178
Flexural Modulus 2.95 GPa428 ksiISO 178
Charpy Impact Unnotched NB
@Temperature 23.0 °C
NB
@Temperature 73.4 °F
ISO 179-1/1eU
Charpy Impact, Notched 0.650 J/cm²
@Temperature 23.0 °C
3.09 ft-lb/in²
@Temperature 73.4 °F
ISO 179-1/1eA
 
Thermal PropertiesMetricEnglishComments
Melting Point >= 180 °C>= 356 °FISO 3146-C
Vicat Softening Point 110 °C230 °FA; ISO 306
 
Descriptive Properties
Melt Volume Flow (cm3/10 min)9-13ISO 1133; 230°C, 5kg

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
FKuR Kunststoff Biograde® C 6509 CL Biodegradable Plastic Compound
Akzo Nobel Injection molding of 20% Wood Plastic Composite with 3.25% Expancel 092-120
FKuR Kunststoff Biograde® C 6530 Biodegradable Plastic Compound
FKuR Kunststoff Biograde® C 9550 Biodegradable Plastic Compound
A. Schulman Diamond DIAMALOY WPE 2000 Wood Filled HDPE

PFKUR007 / 107045

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.