MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

GEHR Plastics PEEK-30GF Polyetheretherketone, 30% Glass Fiber
Categories: Polymer; Thermoplastic; Polyketone; Polyetheretherketone (PEEK); Polyetheretherketone, PEEK, Glass Fiber Filled

Material Notes: Polyether etherketone can be used at very high temperatures and it shows a good mechanical strength, toughness, hardness, flexural strength, and torsional strength. PEEK exhibits excellent chemical resistance, very good dielectric properties up to 260°C and a very good resistance to all kinds of radiation.

Properties:

  • very high mechanical strength
  • very high rigidity
  • very high thermal stability
  • very high creep resistance
  • very high dimensional stability
  • very high radiation resistance
  • very high hydrolysis resistance
  • relatively low notch impact-strength
  • low resistance against acetone
Applications include bearing shells, piston rings, valve seats, gears, seals, aviation, cog-wheels, pump vanes, fittings, plug connectors, and wafer carriers.

Vendors: Ensinger TECAPEEK™ shapes are manufactured exclusively with Victrex™ PEEK polymer. The Ensinger process and Victrex resins ensure reliability, consistency, dimensional stability, and high temperature mechanical performance.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.51 g/cc1.51 g/ccISO 1183
Moisture Absorption at Equilibrium 0.040 %0.040 %ISO 62
Water Absorption at Saturation 0.30 %0.30 %ISO 62
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 9090ISO 868
Ball Indentation Hardness 315 MPa45700 psiISO 2039
Tensile Strength at Break 180 MPa26100 psiISO 527
Tensile Strength, Yield 105 MPa15200 psiISO 527
Elongation at Break 2.7 %2.7 %ISO 527
Elongation at Yield 3.0 %3.0 %ISO 527
Modulus of Elasticity 6.38 GPa925 ksiISO 527
Flexural Strength 164 MPa23800 psiISO 178
Charpy Impact Unnotched 3.20 J/cm²15.2 ft-lb/in²ISO 179
Charpy Impact, Notched 0.800 J/cm²3.81 ft-lb/in²ISO 179
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 3.00e+13 ohm-cm3.00e+13 ohm-cmIEC 60093
Surface Resistance >= 1.00e+13 ohm>= 1.00e+13 ohmIEC 60093
Dielectric Constant 3.2
@Frequency 1e+6 Hz
3.2
@Frequency 1e+6 Hz
IEC 60250
Dielectric Strength 20.0 kV/mm508 kV/inIEC 60243-1
Dielectric Loss Index 0.0050
@Frequency 1e+6 Hz
0.0050
@Frequency 1e+6 Hz
IEC 60250
 
Thermal PropertiesMetricEnglishComments
CTE, linear 38.0 µm/m-°C21.1 µin/in-°FISO 11359
Thermal Conductivity 0.350 W/m-K
@Temperature 20.0 °C
2.43 BTU-in/hr-ft²-°F
@Temperature 68.0 °F
ISO 22007-4
Melting Point 341 °C646 °FDIN EN ISO 3146
Maximum Service Temperature, Air 260 °C500 °FUL 746B
Deflection Temperature at 1.8 MPa (264 psi) 328 °C622 °FISO 75
Glass Transition Temp, Tg 147 °C297 °FDIN EN ISO 3146
Flammability, UL94 V-0V-0UL 94
Oxygen Index 43 %43 %ASTM D2863
 
Compliance PropertiesMetricEnglishComments
FDA NoNoPhysiological indifference
 
Descriptive Properties
Acid Resistanceyes
Aromatic Resistanceyes
Bondabilityyes
CKW Resistancelimited
Colornatural
Hydrocarbonate Resistanceyes
Hydroxide Resistanceyes
Ketone Resistanceyes
Physiological indifferenceno, EEC
Resistance Against Hot Wateryes
UV Stabilizationlimited

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
CRP Technology AMC225xe Aluminum Alloy - SiC Composite, T4 Condition
NRI Trans-Wrap Carbon Fiber Epoxy Composite
Ensinger Tecapeek® XP-101 Compression Molded PEEK Compound, Filled with 15% Graphite and 10% PTFE
Ensinger Tecapeek® XP-102 Compression Molded PEEK Compound, Filled with 15% Graphite and 10% PTFE
GEHR Plastics PEEK-mod Polyetheretherketone, 10% PTFE, 10% Graphite, 10% Carbon Fiber

PGEHR039 / 79876

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.