MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

American Polymers API 375 Polystyrene
Categories: Polymer; Thermoplastic; Polystyrene (PS); Polystyrene, Molded, Unreinforced

Material Notes: API 375 is a general purpose polystyrene produced in pellet form for injection molding. API 375 has excellent strength and clarity as well as fast set-up properties.

Applications: Used in the manufacture of containers, housewares, toys and medical applications.

Information provided by American Polymers, Inc.

Key Words: PS
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.05 g/cc0.0379 lb/in³ASTM D792
Melt Flow 5.0 g/10 min5.0 g/10 minCondition G; ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell L 7676ASTM D785
Tensile Strength, Ultimate 44.5 MPa6450 psiASTM D638
Elongation at Break 1.5 %1.5 %ASTM D638
Tensile Modulus 2.85 GPa413 ksiASTM D638
Izod Impact, Notched 0.160 J/cm
@Thickness 3.17 mm
0.300 ft-lb/in
@Thickness 0.125 in
injection molded sample; ASTM D256
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 1.8 MPa (264 psi) 90.6 °C195 °FAnnealed; ASTM D648
Vicat Softening Point 102 °C215 °FASTM D1525

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Overview of materials for Polystyrene, Molded, Unreinforced
A. Schulman Diamond DIAMALOY 508 30% Glass Filled PC/Polyester Alloy, UV Stabilized
INEOS Styrolution PS 5310 HIPS
Aclo Accucomp Polystyrene HS0600L High Impact
INEOS Styrolution PS 1600 GPPS

PAMER001 / 24002

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.