MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

EMS-Grivory Grilamid® XE 4158 nat PA612  (discontinued **)
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 612 (PA612)

Material Notes: Product description: Grilamid XE 4158 natural is a medium viscosity Polyamide 12 with super high impact strength. The main features of Grilamid XE 4158 natural are:
  • Very good hydrolysis resistance
  • Good heat stability
  • High UV- and weathering resistance
  • Super high cold impact strength
  • Good chemical resistance
  • Good surface finish
  • Good dimensional stability
  • Low density
Grilamid XE 4158 natural is suitable for the extrusion of profiles and tubes for applications in automotive and industrial markets. In addition it can be used for injection molding applications such as winter sport items for which high impact strength at low temperatures is required.

Information provided by EMS Grivory

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.980 g/cc0.0354 lb/in³ISO 1183
Water Absorption 1.3 %1.3 %ISO 62
Moisture Absorption 0.600 %0.600 %ISO 62
Linear Mold Shrinkage, Flow 0.010 cm/cm0.010 in/inISO 294-4, 2577
Linear Mold Shrinkage, Transverse 0.016 cm/cm0.016 in/inISO 294-4, 2577
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 6565dry, 15s; ISO 868
 6565conditioned, 15s; ISO 868
Tensile Strength, Yield 30.0 MPa4350 psiconditioned; ISO 527-1/-2
 30.0 MPa4350 psidry; ISO 527-1/-2
Elongation at Break >= 50 %>= 50 %conditioned; ISO 527-1/-2
 <= 50 %<= 50 %dry; ISO 527-1/-2
Elongation at Yield 13 %13 %dry; ISO 527-1/-2
 18 %18 %conditioned; ISO 527-1/-2
Tensile Modulus 0.750 GPa109 ksiconditioned; ISO 527-1/-2
 1.00 GPa145 ksidry; ISO 527-1/-2
Charpy Impact Unnotched NBNBdry; ISO 179/1eU
 NBNBconditioned; ISO 179/1eU
 NB
@Temperature -30.0 °C
NB
@Temperature -22.0 °F
dry; ISO 179/1eU
 NB
@Temperature -30.0 °C
NB
@Temperature -22.0 °F
conditioned; ISO 179/1eU
Charpy Impact, Notched 8.50 J/cm²40.4 ft-lb/in²dry; ISO 179/1eA
 8.50 J/cm²40.4 ft-lb/in²conditioned; ISO 179/1eA
 4.00 J/cm²
@Temperature -30.0 °C
19.0 ft-lb/in²
@Temperature -22.0 °F
conditioned; ISO 179/1eA
 6.00 J/cm²
@Temperature -30.0 °C
28.6 ft-lb/in²
@Temperature -22.0 °F
dry; ISO 179/1eA
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+11 ohm-cm1.00e+11 ohm-cmdry; IEC 60093
 1.00e+11 ohm-cm1.00e+11 ohm-cmconditioned; IEC 60093
Surface Resistance 1.00e+11 ohm1.00e+11 ohmIEC 60093
Dielectric Strength 40.0 kV/mm1020 kV/indry; IEC 60243-1
 40.0 kV/mm1020 kV/inconditioned; IEC 60243-1
Comparative Tracking Index 600 V600 Vconditioned; IEC 60112
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 170 µm/m-°C94.4 µin/in-°FISO 11359-1/-2
CTE, linear, Transverse to Flow 210 µm/m-°C117 µin/in-°FISO 11359-1/-2
Melting Point 179 °C354 °F10°C/min; ISO 11357-1/-3
Maximum Service Temperature, Air 90.0 - 100 °C194 - 212 °Flong term; EMS
 150 °C302 °Fshort term; EMS
Deflection Temperature at 0.46 MPa (66 psi) 70.0 °C158 °FISO 75-1/-2
Deflection Temperature at 1.8 MPa (264 psi) 45.0 °C113 °FISO 75-1/-2
Flammability, UL94 HBHBIEC 60695-11-10
 
Descriptive Properties
AutomotiveAir intake systems
 Compressed air systems
 Cooling and climate control
Electricals & ElectronicsCables & Tubes
FormGranules
Industry & Consumer goodsHydraulics & Pneumatics
 Sports & Leisure
 Tools & Accessories
ProcessingInjection Molding
 Other Extrusion
Product AttributesFlexible
 Hydrolysis resistant
 Improved alcohol resistance
Special CharacteristicsHigh impact or impact modified
 Improved heat resistance
 Improved UV resistance (outdoor use)

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Arkema Rilsan® Tieflex R463 NAT TL PA
Clariant Renol 612-01L Nylon 612, Lubricated
Evonik VESTAMID® D26 PA 612 Conditioned
EMS-Grivory Grilamid® XE 4208 black 9992 PA612-I
EMS-Grivory Grilamid® XE 4107 nat PA612-GF40

PGRH139 / 156848

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.