MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Westlake Plastics

Overview of materials for Polycarbonate, Gamma Radiation Resistant
Categories: Polymer; Thermoplastic; Polycarbonate (PC); Polycarbonate, Gamma Radiation Resistant

Material Notes: This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Gamma Radiation Resistant". Each property range of values reported is minimum and maximum values of appropriate MatWeb entries. The comments report the average value, and number of data points used to calculate the average. The values are not necessarily typical of any specific grade, especially less common values and those that can be most affected by additives or processing methods.

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 1.19 - 1.21 g/cc0.0430 - 0.0437 lb/in³Average value: 1.20 g/cc Grade Count:50
Water Absorption 0.140 - 0.350 %0.140 - 0.350 %Average value: 0.194 % Grade Count:34
Moisture Absorption at Equilibrium 0.0200 - 0.350 %0.0200 - 0.350 %Average value: 0.195 % Grade Count:33
 0.580 - 0.580 %
@Temperature 100 - 100 °C
0.580 - 0.580 %
@Temperature 212 - 212 °F
Average value: 0.580 % Grade Count:5
Water Absorption at Saturation 0.160 - 0.350 %0.160 - 0.350 %Average value: 0.202 % Grade Count:12
Viscosity  3.00 - 33.0 cP
@Temperature 300 - 330 °C
3.00 - 33.0 cP
@Temperature 572 - 626 °F
Average value: 14.3 cP Grade Count:11
 3.00 - 33.0 cP
@Load 1.20 - 2.16 kg
3.00 - 33.0 cP
@Load 2.65 - 4.76 lb
Average value: 14.3 cP Grade Count:11
Linear Mold Shrinkage 0.00400 - 0.00800 cm/cm0.00400 - 0.00800 in/inAverage value: 0.00623 cm/cm Grade Count:48
Linear Mold Shrinkage, Transverse 0.00400 - 0.00800 cm/cm0.00400 - 0.00800 in/inAverage value: 0.00600 cm/cm Grade Count:13
Melt Flow 3.00 - 35.0 g/10 min3.00 - 35.0 g/10 minAverage value: 14.9 g/10 min Grade Count:49
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell M 70.0 - 85.070.0 - 85.0Average value: 76.0 Grade Count:23
Hardness, Rockwell R 118 - 122118 - 122Average value: 119 Grade Count:30
Ball Indentation Hardness 95.0 MPa13800 psiAverage value: 95.0 MPa Grade Count:6
Tensile Strength, Ultimate 46.9 - 74.0 MPa6800 - 10700 psiAverage value: 66.2 MPa Grade Count:45
Tensile Strength, Yield 59.0 - 65.5 MPa8560 - 9500 psiAverage value: 62.9 MPa Grade Count:50
Elongation at Break 50.0 - 180 %50.0 - 180 %Average value: 114 % Grade Count:50
Elongation at Yield 5.40 - 7.00 %5.40 - 7.00 %Average value: 6.39 % Grade Count:46
Modulus of Elasticity 2.09 - 2.50 GPa303 - 363 ksiAverage value: 2.29 GPa Grade Count:38
Flexural Yield Strength 66.0 - 100 MPa9570 - 14500 psiAverage value: 91.0 MPa Grade Count:46
Flexural Modulus 2.02 - 2.41 GPa293 - 350 ksiAverage value: 2.25 GPa Grade Count:44
Izod Impact 600 - 702 J443 - 518 ft-lbAverage value: 640 J Grade Count:11
 120 - 220 J
@Temperature -30.0 - -30.0 °C
88.5 - 162 ft-lb
@Temperature -22.0 - -22.0 °F
Average value: 151 J Grade Count:11
Izod Impact, Notched 0.981 - 750 J/cm1.84 - 1410 ft-lb/inAverage value: 28.6 J/cm Grade Count:28
 2.20 - 7.85 J/cm
@Temperature -30.0 - -30.0 °C
4.12 - 14.7 ft-lb/in
@Temperature -22.0 - -22.0 °F
Average value: 5.03 J/cm Grade Count:6
Izod Impact, Unnotched 27.0 J/cm - NB50.6 ft-lb/in - NBAverage value: 31.0 J/cm Grade Count:19
Izod Impact, Notched (ISO) 12.0 - 78.0 kJ/m²5.71 - 37.1 ft-lb/in²Average value: 47.5 kJ/m² Grade Count:32
 10.0 - 15.0 kJ/m²
@Temperature -30.0 - -30.0 °C
4.76 - 7.14 ft-lb/in²
@Temperature -22.0 - -22.0 °F
Average value: 11.1 kJ/m² Grade Count:23
Izod Impact, Unnotched (ISO) NBNBGrade Count:22
 NB - NB
@Temperature -30.0 - -30.0 °C
NB - NB
@Temperature -22.0 - -22.0 °F
Grade Count:17
Charpy Impact Unnotched 1000 J/cm² - NB4760 ft-lb/in² - NBGrade Count:20
 999.9 - 999.9 J/cm²
@Temperature -30.0 - -30.0 °C
4759 - 4759 ft-lb/in²
@Temperature -22.0 - -22.0 °F
Grade Count:14
Charpy Impact, Notched 1.00 - 8.20 J/cm²4.76 - 39.0 ft-lb/in²Average value: 4.72 J/cm² Grade Count:35
 1.00 - 1.50 J/cm²
@Temperature -30.0 - -30.0 °C
4.76 - 7.14 ft-lb/in²
@Temperature -22.0 - -22.0 °F
Average value: 1.34 J/cm² Grade Count:17
Gardner Impact 36.2 J26.7 ft-lbAverage value: 36.2 J Grade Count:8
Tensile Impact Strength 378 - 577 kJ/m²180 - 275 ft-lb/in²Average value: 481 kJ/m² Grade Count:21
Dart Drop, Total Energy 54.0 - 149 J39.8 - 110 ft-lbAverage value: 97.4 J Grade Count:27
Falling Dart Impact 169 J125 ft-lbAverage value: 169 J Grade Count:5
Taber Abrasion, mg/1000 Cycles 10.0 - 32.010.0 - 32.0Average value: 12.8 Grade Count:8
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 1.00e+15 - 2.60e+17 ohm-cm1.00e+15 - 2.60e+17 ohm-cmAverage value: 1.20e+17 ohm-cm Grade Count:28
Surface Resistance 1.00e+15 - 6.00e+15 ohm1.00e+15 - 6.00e+15 ohmAverage value: 2.43e+15 ohm Grade Count:14
Dielectric Constant 2.70 - 3.172.70 - 3.17Average value: 2.95 Grade Count:22
Dielectric Strength 14.9 - 35.0 kV/mm378 - 889 kV/inAverage value: 18.4 kV/mm Grade Count:22
Dissipation Factor 0.000100 - 0.02400.000100 - 0.0240Average value: 0.00709 Grade Count:22
Comparative Tracking Index 125 - 250 V125 - 250 VAverage value: 203 V Grade Count:4
High Voltage Arc-Tracking Rate, HVTR 80.0 - 150 mm/min3.15 - 5.91 in/minAverage value: 115 mm/min Grade Count:3
 
Thermal PropertiesMetricEnglishComments
CTE, linear 59.4 - 91.8 µm/m-°C33.0 - 51.0 µin/in-°FAverage value: 69.1 µm/m-°C Grade Count:37
CTE, linear, Transverse to Flow 60.0 - 80.0 µm/m-°C33.3 - 44.4 µin/in-°FAverage value: 68.6 µm/m-°C Grade Count:22
Specific Heat Capacity 1.25 - 1.26 J/g-°C0.299 - 0.301 BTU/lb-°FAverage value: 1.25 J/g-°C Grade Count:14
Thermal Conductivity 0.190 - 0.210 W/m-K1.32 - 1.46 BTU-in/hr-ft²-°FAverage value: 0.202 W/m-K Grade Count:17
Maximum Service Temperature, Air 120 °C248 °FAverage value: 120 °C Grade Count:4
Hot Ball Pressure Test 75.0 - 140 °C167 - 284 °FAverage value: 117 °C Grade Count:16
Deflection Temperature at 0.46 MPa (66 psi) 124 - 145 °C255 - 293 °FAverage value: 136 °C Grade Count:32
Deflection Temperature at 1.8 MPa (264 psi) 117 - 143 °C243 - 289 °FAverage value: 129 °C Grade Count:47
Vicat Softening Point 137 - 160 °C279 - 320 °FAverage value: 147 °C Grade Count:42
Minimum Service Temperature, Air -40.0 °C-40.0 °FAverage value: -40.0 °C Grade Count:4
UL RTI, Electrical 80.0 - 125 °C176 - 257 °FAverage value: 114 °C Grade Count:4
UL RTI, Mechanical with Impact 80.0 - 125 °C176 - 257 °FAverage value: 114 °C Grade Count:4
UL RTI, Mechanical without Impact 80.0 - 125 °C176 - 257 °FAverage value: 114 °C Grade Count:4
Flammability, UL94 HB - V-2HB - V-2Grade Count:16
Oxygen Index 25.0 %25.0 %Average value: 25.0 % Grade Count:8
Glow Wire Test 850 °C1560 °FAverage value: 850 °C Grade Count:3
 
Optical PropertiesMetricEnglishComments
Refractive Index 1.59 - 1.601.59 - 1.60Average value: 1.59 Grade Count:20
Haze 0.600 - 3.00 %0.600 - 3.00 %Average value: 1.11 % Grade Count:31
Transmission, Visible 82.0 - 89.0 %82.0 - 89.0 %Average value: 86.3 % Grade Count:24
UV Transmittance 88.0 %88.0 %Average value: 88.0 % Grade Count:8
 
Processing PropertiesMetricEnglishComments
Processing Temperature 60.0 - 80.0 °C140 - 176 °FAverage value: 70.0 °C Grade Count:6
Nozzle Temperature 265 - 355 °C509 - 671 °FAverage value: 304 °C Grade Count:25
Melt Temperature 249 - 360 °C480 - 680 °FAverage value: 299 °C Grade Count:33
Mold Temperature 65.6 - 116 °C150 - 240 °FAverage value: 89.2 °C Grade Count:33
Drying Temperature 118 - 124 °C245 - 255 °FAverage value: 120 °C Grade Count:33
Moisture Content 0.0200 %0.0200 %Average value: 0.0200 % Grade Count:14
Vent Depth 0.00127 - 0.00760 cm0.000500 - 0.00299 inAverage value: 0.00393 cm Grade Count:27

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Overview of materials for Polycarbonate, Glass Fiber Filled, Flame Retardant
Overview of materials for Polycarbonate, 10% Glass Filled
Overview of materials for Polycarbonate, PTFE Filled
Overview of materials for Polycarbonate, UV Stabilized
Overview of materials for Polycarbonate, Optical Grade

O3109 / 78128

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.