MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Akro-Plastic Akromid® T1 GF 50 natural (3376) PPA Dry, 50% Glass Filled
Categories: Polymer; Thermoplastic; Polyphthalamide (PPA); Polyphthalamide (PPA), 50% Glass Fiber Reinforced

Material Notes: Description: AKROMID T1 GF 50 natural (3376) is a 50% glass fiber reinforced polyphthalamide with very high rigidity and strength, as well as high temperature and chemical resistance and light inherent color.

Features:

  • Good Chemical Resistance
  • High Stiffness
  • High Strength
  • High Heat Resistance

Information provided by Akro-Plastic GmbH

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.62 g/cc0.0585 lb/in³ISO 1183
Filler Content 50 %50 %ISO 1172
Moisture Absorption 0.85 %
@Temperature 70.0 °C
0.85 %
@Temperature 158 °F
Humidity, 62% RH; ISO 1110
Linear Mold Shrinkage, Flow 0.0030 cm/cm0.0030 in/inISO 294-4
Linear Mold Shrinkage, Transverse 0.0070 cm/cm0.0070 in/inISO 294-4
 
Mechanical PropertiesMetricEnglishComments
Ball Indentation Hardness 360 MPa52200 psiH 961/30; ISO 2039-1
Tensile Strength at Break 270 MPa39200 psi5 [mm/min]; ISO 527-2
 140 MPa
@Treatment Temp. 170 - 180 °C,
Time 1.80e+7 sec
20300 psi
@Treatment Temp. 338 - 356 °F,
Time 5000 hour
50% Loss of Tensile Strength
 140 MPa
@Treatment Temp. 170 - 180 °C,
Time 7.20e+7 sec
20300 psi
@Treatment Temp. 338 - 356 °F,
Time 20000 hour
50% Loss of Tensile Strength
Elongation at Break 2.0 %2.0 %5 [mm/min]; ISO 527-2
Tensile Modulus 20.0 GPa2900 ksi1 [mm/min]; ISO 527-2
Flexural Strength 380 MPa55100 psi2 [mm/min]; ISO 178
Flexural Modulus 18.0 GPa2610 ksi2 [mm/min]; ISO 178
Flexural Strain at Break 2.4 %2.4 %2 mm/min; ISO 178
Charpy Impact, Notched  7.00 J/cm²
@Temperature -30.0 °C
33.3 ft-lb/in²
@Temperature -22.0 °F
ISO 179/1eA
 9.00 J/cm²
@Temperature 23.0 °C
42.8 ft-lb/in²
@Temperature 73.4 °F
ISO 179/1eA
 
Electrical PropertiesMetricEnglishComments
Comparative Tracking Index 600 V600 VSolution A; IEC 60112
 
Thermal PropertiesMetricEnglishComments
Melting Point 313 °C595 °FDIN EN 11357-1
Deflection Temperature at 0.46 MPa (66 psi) 310 °C590 °FUnannealed; ISO 75/B
Deflection Temperature at 1.8 MPa (264 psi) 285 °C545 °FUnannealed; ISO 75/A
Deflection Temperature at 8.0 MPa 230 °C446 °FUnannealed; ISO 75/C
Flammability, UL94 HB
@Thickness 0.800 mm
HB
@Thickness 0.0315 in
Glow Wire Flammability Index 960 °C
@Thickness 3.20 mm
1760 °F
@Thickness 0.126 in
IEC 60695-2-12

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Overview of materials for Polyphthalamide (PPA)
Akro-Plastic Akromid® T1 GF 50 9 (3257) PPA Dry, 50% Glass Filled
Akro-Plastic Akromid® T1 GF 50 9 (3257) PPA Conditioned, 50% Glass Filled
Akro-Plastic Akromid® T1 GF 50 (3101) PPA Conditioned, 50% Glass Filled
Overview of materials for Polyphthalamide (PPA), 30% Glass Fiber Reinforced

PAKRO368 / 182955

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.