MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Avient Maxxam™ FR JS8830-23 Polypropylene  (discontinued **)
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene, Molded

Material Notes: Typical Properties of Molded Slab (0.075"); Not to be Construed as Specifications.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.25 g/cc1.25 g/ccASTM D792
Melt Flow 48 g/10 min
@Load 2.16 kg,
Temperature 190 °C
48 g/10 min
@Load 4.76 lb,
Temperature 374 °F
Procedure A; ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 17.2 MPa2490 psiType IV, 510 mm/min; ASTM D638
Elongation at Break 550 %550 %Type IV, 510 mm/min; ASTM D638
 
Electrical PropertiesMetricEnglishComments
Dielectric Constant 2.38
@Frequency 1000 Hz
2.38
@Frequency 1000 Hz
ASTM D150
Dissipation Factor 0.0030
@Frequency 1000 Hz
0.0030
@Frequency 1000 Hz
ASTM D150
 
Thermal PropertiesMetricEnglishComments
Oxygen Index 27 %
@Thickness 1.91 mm
27 %
@Thickness 0.0752 in
ASTM D2863
 
Descriptive Properties
FeaturesFlame Retardant
 Foamable
FormsPellets
Processing MethodExtrusion Coating
Regional AvailabilityAfrica & Middle East
 Asia Pacific
 Europe
 North America
 South America
Retention of Elongation, %80168 hr, UL Standard; 113°C, 1.91 mm
Retention of Tensile Strength, %100168 hr, UL Standard; 113°C, 1.91 mm
UsesCommunication Wire Insulation
 Foam
 Insulation
 Wire & Cable Applications
Wire TypesCL2
 CM
 CMR
 FT-4

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Avient Maxxam® FR PE 125 Low Density Polyethylene, Wire and Cable
Avient Maxxam® FR PE 113 Low Density Polyethylene (LDPE)
AlphaGary Smokeguard™ O 301 Low Smoke Halogen Free
AlphaGary Smokeguard™ O 405 Low Smoke Halogen Free

PH1PN9119 / 102955

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.