MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

NOVA Chemicals Sclair® 2815 HDPE Injection Molding Resin
Categories: Polymer; Thermoplastic; Polyethylene (PE); High Density (HDPE); High Density Polyethylene (HDPE), Injection Molded

Material Notes: Features: Excellent balance of stiffness and toughness, low odor.

Applications: Margarine and spreads, thin walled containers, frozen food containers.

Data provided by the manufacturer.

Key Words: High Density Polyethylene
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.954 g/cc0.0345 lb/in³ASTM D792
Apparent Bulk Density 0.610 g/cc0.0220 lb/in³
Melt Flow 67 g/10 min
@Load 2.16 kg,
Temperature 190 °C
67 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Spiral Flow 38.0 cm15.0 inNOVA Snake Flow Test
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 6363ASTM D2240
Tensile Strength, Yield 27.0 MPa3920 psiASTM D638
Flexural Modulus 1.07 GPa155 ksiASTM D790
 
Thermal PropertiesMetricEnglishComments
Vicat Softening Point 123 °C253 °FASTM D1525
 
Processing PropertiesMetricEnglishComments
Melt Temperature 170 - 260 °C338 - 500 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Dow DOWLEX™ IP-90 High Density Polyethylene
Dow DMDA-8980 NT 7 High Density Polyethylene Resin
Dow HDPE 65053N High Density Polyethylene
Chevron Phillips Marlex® 9004 HDPE Injection Molding Resin
Chevron Phillips Marlex® 9035 High Density Polyethylene, Injection Molding

PEHN1V / 35580

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.