MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

INEOS Styrolution Terluran® EGP-7 ABS
Categories: Polymer; Thermoplastic; ABS Polymer; Acrylonitrile Butadiene Styrene (ABS), Extruded

Material Notes: Terluran EGP-7 is an extrusion grade with well balanced properties.
  • UL 94 HB

Information provided by Styrolution

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.03 g/cc0.0372 lb/in³ISO 1183
Moisture Absorption at Equilibrium 0.21 %
@Temperature 23.0 °C
0.21 %
@Temperature 73.4 °F
50% RH; ISO 62
Water Absorption at Saturation 0.95 %
@Temperature 23.0 °C
0.95 %
@Temperature 73.4 °F
ISO 62
Linear Mold Shrinkage 0.0040 - 0.0070 cm/cm0.0040 - 0.0070 in/inISO 294-4
Melt Flow 5.0 g/10 min
@Load 10.0 kg,
Temperature 220 °C
5.0 g/10 min
@Load 22.0 lb,
Temperature 428 °F
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Ball Indentation Hardness 97.0 MPa14100 psiISO 2039-1
Tensile Strength, Yield 43.0 MPa6240 psiISO 527
Elongation at Yield 2.9 %2.9 %ISO 527
Tensile Modulus 2.40 GPa348 ksiISO 527
Flexural Strength 65.0 MPa9430 psiISO 178
Flexural Modulus 2.00 GPa290 ksiISO 178
Izod Impact, Notched (ISO)  14.0 kJ/m²
@Temperature -30.0 °C
6.66 ft-lb/in²
@Temperature -22.0 °F
ISO 180/A
 34.0 kJ/m²
@Temperature 23.0 °C
16.2 ft-lb/in²
@Temperature 73.4 °F
ISO 180/A
Charpy Impact Unnotched NBNBISO 179
Charpy Impact, Notched  1.40 J/cm²
@Temperature -30.0 °C
6.66 ft-lb/in²
@Temperature -22.0 °F
ISO 179
 3.30 J/cm²
@Temperature 23.0 °C
15.7 ft-lb/in²
@Temperature 73.4 °F
ISO 179
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity >= 1.00e+15 ohm-cm>= 1.00e+15 ohm-cmIEC 60093
 
Thermal PropertiesMetricEnglishComments
CTE, linear 80.0 - 110 µm/m-°C44.4 - 61.1 µin/in-°FISO 11359
Thermal Conductivity 0.170 W/m-K1.18 BTU-in/hr-ft²-°FDIN 52612-1
Maximum Service Temperature, Air 80.0 °C176 °F
Deflection Temperature at 0.46 MPa (66 psi) 103 °C217 °FISO 75
Deflection Temperature at 1.8 MPa (264 psi) 101 °C214 °FISO 75
Vicat Softening Point  100 °C
@Load 5.10 kg
212 °F
@Load 11.2 lb
50°C/h; ISO 306
 107 °C
@Load 1.02 kg
225 °F
@Load 2.25 lb
50°C/h; ISO 306
Flammability, UL94 HBHB
 
Processing PropertiesMetricEnglishComments
Melt Temperature 203 - 250 °C397 - 482 °FISO 294

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
INEOS Styrolution Terluran® GP-22 ABS
INEOS Styrolution Terluran® GP-25 ABS
INEOS Styrolution Terluran® HI-10 ABS
LyondellBasell Pro-fax SG702 Polypropylene Impact Copolymer
Albis Plastics ABS 01A HI01 Unreinforced

PBASF9048D / 159690

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.