Product Profile: PLEXIGLAS® Heatstop 8N black is an amorphous thermoplastic molding compound (PMMA). Typical properties of PLEXIGLAS® molding compounds are:- good flow
- high mechanical strength, surface hardness and abrasion resistance
- very good weather resistance
Special properties of PLEXIGLAS® Heatstop 8N black are:- heat-reflection (IR)
- high total solar reflection (TSR), reflects 21% of the solar energy
- reduces the heat build-up of plastic parts, thus increases the dimension stability.
Application: PLEXIGLAS® Heatstop 8N black is suitable for injection molding of technical components, as well as for extrusion/coextrusion. Owing to its superior brilliance, high-gloss (Class A) black surfaces can be obtained.The former Evonik Methacrylates business has been sold to Röhm GmbH (Roehm). |