MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Celanese Hostaform® S 9363 POM, Impact Modified
Categories: Polymer; Thermoplastic; Acetal (Polyoxymethylene, POM); Acetal Copolymer, Impact Modified

Material Notes: Hostaform« acetal copolymer grade S 9363 is an impact modified grade for demanding applications. Hostaform« S 9363 provides good impact strength while improving modulus and weld line strength over standard impact modified grades such as Hostaform« S 9064.

Information provided by Celanese

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.38 g/cc0.0499 lb/in³ISO 1183
Water Absorption at Saturation 0.80 %0.80 %ISO 62
Linear Mold Shrinkage, Flow 0.018 cm/cm0.018 in/inISO 294-4
Linear Mold Shrinkage, Transverse 0.016 cm/cm0.016 in/inISO 294-4
Melt Flow 5.5 g/10 min
@Load 2.16 kg,
Temperature 190 °C
5.5 g/10 min
@Load 4.76 lb,
Temperature 374 °F
[cm3/10min]; ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 50.0 MPa7250 psi50mm/min; ISO 527-2/1A
Elongation at Yield 12 %12 %50mm/min; ISO 527-2/1A
Tensile Modulus 2.00 GPa290 ksi50mm/min; ISO 527-2/1A
Flexural Modulus 2.00 GPa290 ksiISO 178
Charpy Impact Unnotched NBNBISO 179/1eU
 NB
@Temperature -30.0 °C
NB
@Temperature -22.0 °F
ISO 179/1eU
Charpy Impact, Notched 1.30 J/cm²6.19 ft-lb/in²ISO 179/1eA
 0.800 J/cm²
@Temperature -30.0 °C
3.81 ft-lb/in²
@Temperature -22.0 °F
ISO 179/1eA
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 110 µm/m-°C61.1 µin/in-°FISO 11359-2
CTE, linear, Transverse to Flow 110 µm/m-°C61.1 µin/in-°FISO 11359-2
Melting Point 166 °C331 °F10°C/min; ISO 11357-1,-2,-3
Deflection Temperature at 0.46 MPa (66 psi) 148 °C298 °FISO 75-1, -2
Deflection Temperature at 1.8 MPa (264 psi) 84.0 °C183 °FISO 75-1, -2
 
Processing PropertiesMetricEnglishComments
Processing Temperature 60.0 - 70.0 °C140 - 158 °Fcavity
Zone 1 170 - 180 °C338 - 356 °F
Zone 2 180 - 190 °C356 - 374 °F
Zone 3 180 - 190 °C356 - 374 °F
Zone 4 180 - 200 °C356 - 392 °F
Die Temperature 180 - 200 °C356 - 392 °F
Melt Temperature 180 - 200 °C356 - 392 °F
Drying Temperature 80.0 - 100 °C176 - 212 °F
Dry Time 3.00 hour3.00 hour
Injection Pressure 60.0 - 120 MPa8700 - 17400 psi
Hold Pressure 60.0 - 120 MPa8700 - 17400 psi
Back Pressure <= 2.00 MPa<= 290 psi
 
Descriptive Properties
Injection moldingYes
Injection speedslow
Processing conditions acc. ISO9988-2
Profile extrusionYes

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Celanese Hostaform® S 9363 XAP² ™ POM, Impact Modified
Celanese Hostaform® C 13031 LS POM, UV Resistant
Celanese Hostaform® C 27021 POM, Unfilled
Celanese Hostaform® C 13031 POM, Unfilled
Celanese Hostaform® C 9021 GV1/30 POM, 30% Glass Reinforced

PHCQ421 / 178876

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.