MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Celanese Zytel® HTN51G15HSL NC010 PA6T/XT-GF15
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6); Nylon 6, 20% Glass Fiber Filled

Material Notes: 15% Glass Reinforced, PPA, High Performance Polyamide

Former DuPont product acquired by Celanese in 2022.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.30 g/cc0.0470 lb/in³DAM; ISO 1183
Moisture Absorption 2.00 %
@Thickness 2.00 mm
2.00 %
@Thickness 0.0787 in
DAM; Sim. to ISO 62
Linear Mold Shrinkage, Flow 0.0040 cm/cm0.0040 in/inDAM; ISO 294-4, 2577
Linear Mold Shrinkage, Transverse 0.0070 cm/cm0.0070 in/inDAM; ISO 294-4, 2577
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 120 MPa17400 psiDAM; ISO 527-1/-2
Elongation at Break 2.1 %2.1 %DAM; ISO 527-1/-2
Tensile Modulus 6.50 GPa943 ksiDAM; ISO 527-1/-2
Flexural Modulus 5.70 GPa827 ksiDAM; ISO 178
Poissons Ratio 0.350.35DAM
Izod Impact, Notched (ISO)  6.00 kJ/m²
@Temperature -40.0 °C
2.86 ft-lb/in²
@Temperature -40.0 °F
DAM; ISO 180/1A
 6.00 kJ/m²
@Temperature 23.0 °C
2.86 ft-lb/in²
@Temperature 73.4 °F
DAM; ISO 180/1A
Charpy Impact Unnotched  2.00 J/cm²
@Temperature -30.0 °C
9.52 ft-lb/in²
@Temperature -22.0 °F
DS; DAM; ISO 179/1eU
 2.50 J/cm²
@Temperature 23.0 °C
11.9 ft-lb/in²
@Temperature 73.4 °F
DAM; ISO 179/1eU
Charpy Impact, Notched  0.600 J/cm²
@Temperature -30.0 °C
2.86 ft-lb/in²
@Temperature -22.0 °F
DAM; ISO 179/1eA
 0.600 J/cm²
@Temperature 23.0 °C
2.86 ft-lb/in²
@Temperature 73.4 °F
DAM; ISO 179/1eA
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity >= 1.00e+15 ohm-cm>= 1.00e+15 ohm-cmDAM; IEC 62631-3-1
Surface Resistance >= 1.00e+15 ohm>= 1.00e+15 ohm50% RH; IEC 62631-3-2
Comparative Tracking Index 600 V600 VDAM; IEC 60112
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 30.0 µm/m-°C16.7 µin/in-°FDAM; ISO 11359-1/-2
 30.0 µm/m-°C
@Temperature -40.0 - 23.0 °C
16.7 µin/in-°F
@Temperature -40.0 - 73.4 °F
DAM; ISO 11359-1/-2
CTE, linear, Transverse to Flow 64.0 µm/m-°C35.6 µin/in-°FDAM; ISO 11359-1/-2
 57.0 µm/m-°C
@Temperature -40.0 - 23.0 °C
31.7 µin/in-°F
@Temperature -40.0 - 73.4 °F
DAM; ISO 11359-1/-2
 77.0 µm/m-°C
@Temperature 55.0 - 160 °C
42.8 µin/in-°F
@Temperature 131 - 320 °F
DAM; ISO 11359-1/-2
Melting Point 300 °C572 °Ffirst heat; DAM; ISO 11357-1/-3
Deflection Temperature at 0.46 MPa (66 psi) 276 °C529 °FDAM; ISO 75-1/-2
Deflection Temperature at 1.8 MPa (264 psi) 254 °C489 °FDAM; ISO 75-1/-2
Glass Transition Temp, Tg 95.0 °C203 °F10°C/min; 50% RH; ISO 11357-1/-2
 135 °C275 °F10°C/min; DAM; ISO 11357-1/-2
Flammability, UL94  HB
@Thickness 0.750 mm
HB
@Thickness 0.0295 in
DAM; IEC 60695-11-10
 HB
@Thickness 1.50 mm
HB
@Thickness 0.0591 in
DAM; IEC 60695-11-10
Flame Spread 18.0 mm/min
@Thickness 1.00 mm
0.709 in/min
@Thickness 0.0394 in
ISO 3795 (FMVSS 302)
Oxygen Index 23 %23 %DAM; ISO 4589-1/-2
 
Processing PropertiesMetricEnglishComments
Melt Temperature 325 °C617 °FOptimum, Injection
 320 - 330 °C608 - 626 °FRange, Injection
Mold Temperature 150 °C302 °FOptimum, Injection
 140 - 180 °C284 - 356 °FInjection; higher temperature needed for thinner sections
Drying Temperature 100 °C212 °FInjection
Dry Time 6.00 - 8.00 hour6.00 - 8.00 hourInjection, Dehumidified Dryer
Moisture Content <= 0.10 %<= 0.10 %Injection
 
Descriptive Properties
AdditivesRelease agent
Drying RecommendedyesInjection
FMVSS ClassBISO 3795 (FMVSS 302)
ISO designationISO 16396-PA6T/XT,GF15,M1GHNR,S10-060
Part Marking Code>PA6T/XT-GF15<ISO 11469
 >PPA-GF15<SAE J1344
PolymerPA6T/XT-GF15
Resin IdentificationPA6T/XT-GF15ISO 1043

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Celanese Zytel® 73G15L NC010 PA6-GF15
Ravago Manufacturing Americas Hylon N2015STHL Nylon 6, 15% Glass Filled, Superior Toughness, DAM
Ravago Manufacturing Americas Hylon N2015THL Nylon 6, 15% Glass Filled, Impact Modified, DAM
Ravago Manufacturing Americas Hylon N2215STHL Nylon 6, 15% Glass Filled, Superior Toughness, DAM
Ravago Manufacturing Americas Hylon N2215STHLUV2BK Nylon 6, 15% Glass Filled, Superior Toughness, Heat Stabilized, Lubricated, UV Stabilized, DAM

PDSX5431 / 198071

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.