MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Akro-Plastic Akromid® A3 1 S3 black (1139) PA 66, Impact Resistant, Heat Stabilized, Conditioned
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66); Nylon 66, Heat Stabilized; Nylon 66, Impact Grade

Material Notes: Description: AKROMID A3 15 1 black is a 15% glass fiber reinforced, heat stabilized polyamide 6.6 with medium stiffness and strength. Applications are components and housings mainly in mechanical engineering and in the automotive industry.

Additive: Heat Stabilizer

Features:

  • Good Stiffness
  • Heat Stabilized
  • Medium Strength
Uses:
  • Automotive Applications
  • Engineering Parts
  • Housings

Information provided by Akro-Plastic GmbH

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.10 g/cc0.0397 lb/in³ISO 1183
Moisture Absorption 2.1 %
@Temperature 70.0 °C
2.1 %
@Temperature 158 °F
Humidity, 62% RH; ISO 1110
Linear Mold Shrinkage, Flow 0.021 cm/cm0.021 in/inISO 294-4
Linear Mold Shrinkage, Transverse 0.022 cm/cm0.022 in/inISO 294-4
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 45.0 MPa6530 psi50 [mm/min]; ISO 527-2
Elongation at Break >= 100 %>= 100 %50 [mm/min]; ISO 527-2
Tensile Modulus 1.30 GPa189 ksi1 [mm/min]; ISO 527-2
Charpy Impact Unnotched NB
@Temperature 23.0 °C
NB
@Temperature 73.4 °F
ISO 179/1eU
Charpy Impact, Notched  1.30 J/cm²
@Temperature -30.0 °C
6.19 ft-lb/in²
@Temperature -22.0 °F
ISO 179/1eA
 2.50 J/cm²
@Temperature 23.0 °C
11.9 ft-lb/in²
@Temperature 73.4 °F
ISO 179/1eA
 
Thermal PropertiesMetricEnglishComments
Melting Point 262 °C504 °FDIN EN 11357-1
 
Descriptive Properties
Resistance to Fruit JuicesPass50°C, 100% Conc
Resistance to SpiritsPass100% Conc
Resistance to TolueneFail100% Conc
Resistant to Citric acidPass10% Conc
Resistant to Hydrogen peroxideFail
Resistant to Sulfuric acidFail96% Conc
Resistant to WaterPass<50°C, 100% Conc
Resistant to Zinc chloride, aqueousPass50% Conc

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Borealis Daplen™ EH104AE Polypropylene TPO Compound
Akro-Plastic Akromid® A3 1 S3 black (1139) PA 66, Impact Resistant, Heat Stabilized, Dry
BASF Ultramid® B27 E 01 PA6 (Conditioned)
BASF Ultramid® B27 E PA6
BASF Ultramid® B27 E 01 PA6 (Dry)

PAKRO371 / 182958

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.