MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Overview of materials for Acetal Homopolymer, PTFE-Filled
Categories: Polymer; Thermoplastic; Acetal (Polyoxymethylene, POM); Acetal Homopolymer, PTFE-Filled

Material Notes: This property data is a summary of similar materials in the MatWeb database for the category "Acetal Homopolymer, PTFE-Filled". Each property range of values reported is minimum and maximum values of appropriate MatWeb entries. The comments report the average value, and number of data points used to calculate the average. The values are not necessarily typical of any specific grade, especially less common values and those that can be most affected by additives or processing methods.

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 1.42 - 1.55 g/cc0.0513 - 0.0560 lb/in³Average value: 1.50 g/cc Grade Count:39
Water Absorption 0.0100 - 0.300 %0.0100 - 0.300 %Average value: 0.174 % Grade Count:21
Moisture Absorption at Equilibrium 0.110 - 0.200 %0.110 - 0.200 %Average value: 0.150 % Grade Count:8
Water Absorption at Saturation 0.720 - 1.00 %0.720 - 1.00 %Average value: 0.907 % Grade Count:3
Additive Loading 5.00 - 20.0 %5.00 - 20.0 %Average value: 15.0 % Grade Count:3
Linear Mold Shrinkage 0.0100 - 0.0300 cm/cm0.0100 - 0.0300 in/inAverage value: 0.0226 cm/cm Grade Count:18
Linear Mold Shrinkage, Transverse 0.0210 - 0.0260 cm/cm0.0210 - 0.0260 in/inAverage value: 0.0226 cm/cm Grade Count:4
Melt Flow 4.00 - 13.0 g/10 min4.00 - 13.0 g/10 minAverage value: 6.14 g/10 min Grade Count:7
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell M 77.0 - 87.077.0 - 87.0Average value: 81.5 Grade Count:8
Hardness, Rockwell R 79.0 - 12279.0 - 122Average value: 105 Grade Count:14
Hardness, Shore D 79.0 - 83.079.0 - 83.0Average value: 80.9 Grade Count:4
Tensile Strength, Ultimate 41.4 - 64.8 MPa6000 - 9400 psiAverage value: 54.1 MPa Grade Count:24
Tensile Strength, Yield 41.4 - 69.0 MPa6000 - 10000 psiAverage value: 51.0 MPa Grade Count:19
Elongation at Break 3.00 - 22.0 %3.00 - 22.0 %Average value: 11.7 % Grade Count:29
Elongation at Yield 4.00 - 22.0 %4.00 - 22.0 %Average value: 10.7 % Grade Count:10
Modulus of Elasticity 1.55 - 3.28 GPa225 - 475 ksiAverage value: 2.52 GPa Grade Count:23
Flexural Yield Strength 62.1 - 99.3 MPa9000 - 14400 psiAverage value: 80.5 MPa Grade Count:32
Flexural Modulus 2.07 - 3.41 GPa300 - 495 ksiAverage value: 2.75 GPa Grade Count:35
Compressive Yield Strength 8.27 - 96.5 MPa1200 - 14000 psiAverage value: 56.6 MPa Grade Count:9
Compressive Modulus 1.38 - 2.07 GPa200 - 300 ksiAverage value: 1.78 GPa Grade Count:7
Izod Impact, Notched 0.270 - 1.07 J/cm0.506 - 2.00 ft-lb/inAverage value: 0.529 J/cm Grade Count:32
Izod Impact, Unnotched 0.320 - 13.3 J/cm0.600 - 25.0 ft-lb/inAverage value: 4.81 J/cm Grade Count:18
Izod Impact, Notched (ISO) 4.00 - 4.50 kJ/m²1.90 - 2.14 ft-lb/in²Average value: 4.33 kJ/m² Grade Count:3
Izod Impact, Unnotched (ISO) 29.7 - 45.2 kJ/m²14.1 - 21.5 ft-lb/in²Average value: 38.0 kJ/m² Grade Count:3
Falling Dart Impact 5.20 - 7.20 J3.84 - 5.31 ft-lbAverage value: 6.27 J Grade Count:3
Instrumented Impact Total Energy 0.770 - 0.960 J0.568 - 0.708 ft-lbAverage value: 0.850 J Grade Count:3
Coefficient of Friction 0.0700 - 0.3000.0700 - 0.300Average value: 0.191 Grade Count:9
Coefficient of Friction, Static 0.0700 - 0.1800.0700 - 0.180Average value: 0.118 Grade Count:5
K (wear) Factor 18.1 - 121 x 10-8 mm³/N-M9.00 - 60.0 x 10-10 in³-min/ft-lb-hrAverage value: 46.1 x 10-8 mm³/N-M Grade Count:8
Limiting Pressure Velocity 0.0560 - 0.420 MPa-m/sec1600 - 12000 psi-ft/minAverage value: 0.247 MPa-m/sec Grade Count:5
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 1.00e+14 - 1.00e+16 ohm-cm1.00e+14 - 1.00e+16 ohm-cmAverage value: 1.90e+15 ohm-cm Grade Count:16
Surface Resistance 1.00e+13 - 1.00e+16 ohm1.00e+13 - 1.00e+16 ohmAverage value: 2.21e+15 ohm Grade Count:5
Dielectric Constant 3.10 - 3.603.10 - 3.60Average value: 3.30 Grade Count:5
Dielectric Strength 15.7 - 20.0 kV/mm400 - 508 kV/inAverage value: 18.0 kV/mm Grade Count:9
Dissipation Factor 0.00300 - 0.01000.00300 - 0.0100Average value: 0.00725 Grade Count:4
 
Thermal PropertiesMetricEnglishComments
CTE, linear 10.8 - 122 µm/m-°C6.00 - 68.0 µin/in-°FAverage value: 91.5 µm/m-°C Grade Count:10
 91.8 - 91.8 µm/m-°C
@Temperature 29.4 - 60.0 °C
51.0 - 51.0 µin/in-°F
@Temperature 85.0 - 140 °F
Average value: 91.8 µm/m-°C Grade Count:1
Melting Point 119 - 180 °C247 - 356 °FAverage value: 171 °C Grade Count:20
Maximum Service Temperature, Air 82.2 - 150 °C180 - 302 °FAverage value: 109 °C Grade Count:12
Deflection Temperature at 0.46 MPa (66 psi) 73.9 - 171 °C165 - 340 °FAverage value: 153 °C Grade Count:19
Deflection Temperature at 1.8 MPa (264 psi) 93.3 - 168 °C200 - 334 °FAverage value: 111 °C Grade Count:37
Flammability, UL94 HBHBGrade Count:16
 
Processing PropertiesMetricEnglishComments
Melt Temperature 182 - 218 °C360 - 425 °FAverage value: 203 °C Grade Count:18
Mold Temperature 40.0 - 107 °C104 - 225 °FAverage value: 80.8 °C Grade Count:18
Drying Temperature 71.0 - 121 °C160 - 250 °FAverage value: 95.8 °C Grade Count:18
Moisture Content 0.150 %0.150 %Average value: 0.150 % Grade Count:7
Dew Point -31.7 °C-25.0 °FAverage value: -31.7 °C Grade Count:7
Injection Pressure 68.9 - 103 MPa10000 - 15000 psiAverage value: 86.2 MPa Grade Count:7

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Mitsubishi Chemical Advanced Materials Delrin® 100 AF Acetal Extruded Teflon® Filled Acetal
Overview of materials for Acetal Homopolymer, Unreinforced
Ensinger NORYL® Polyphenylene oxide (PPO)
Overview of materials for Acetal Homopolymer, Glass Fiber Reinforced
Overview of materials for Acetal Copolymer, Aramid Fiber Filled

O1288 / 77857

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.