MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Owens Corning Glass Fiber Reinforced Acrylonitrile Butadiene Styrene (ABS), 20 wt.% glass
Categories: Polymer; Thermoplastic; ABS Polymer; Acrylonitrile Butadiene Styrene (ABS), 20% Glass Fiber Filled

Material Notes: ABS is highly resistant to weak acids and alkalis, and provides good resistance to most organic solvents. It is attacked by sulfuric and nitric acids, and is soluble in esters, ketones and ethylene dichloride. Acetal is highly resistant to strong alkalis. Most organic solvents do not seriously alter its properties (test before use). It is not recommended for use in strong acids. Data provided by the manufacturer, Owens Corning.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.22 g/cc0.0441 lb/in³ASTM D792
Water Absorption 0.30 %0.30 %24 hrs.; ASTM D570
Linear Mold Shrinkage 0.0020 cm/cm0.0020 in/inASTM D955
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 107107ASTM D785
Tensile Strength, Ultimate 76.0 MPa11000 psiASTM D638
Elongation at Break 2.0 %2.0 %ASTM D638
Modulus of Elasticity 6.00 GPa870 ksiASTM D638
Flexural Strength 107 MPa15500 psiASTM D790
Flexural Modulus 6.00 GPa870 ksiASTM D790
Compressive Strength 97.0 MPa14100 psiASTM D695
Izod Impact, Notched 0.640 J/cm1.20 ft-lb/in
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+15 ohm-cm1.00e+15 ohm-cmASTM D257
Dielectric Constant 3.2
@Frequency 60 Hz
3.2
@Frequency 60 Hz
ASTM D150
Dielectric Strength 18.3 kV/mm465 kV/inASTM D149
Arc Resistance 80 sec80 secASTM D495
 
Thermal PropertiesMetricEnglishComments
Flammability, UL94 HBHB

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Mitsubishi Chemical Advanced Materials TIVAR® ECO UHMW-PE, UV Resistant (ASTM Product Data Sheet)
LATI Latilub 37 B01-02S Bio-Polymer
Mitsubishi Chemical Advanced Materials TIVAR® ECO UHMW-PE, Recycled (ASTM Product Data Sheet)
INEOS Styrolution Novodur® HD M203FC G3 Acrylonitrile Butadiene Styrene (ABS)
Avient Edgetek® NL-20GF/000 Nylon 6/12, Glass Filled

POC018 / 55596

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.