MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Armacell AP/Armaflex® Black LapSeal™ Tube Insulation with Reinforced Lap Seal
Categories: Other Engineering Material

Material Notes: The original flexible elastomeric pipe insulation with a new and improved lap seal for greater seam security and increased protection against condensation, mold and energy loss.
  • Angled cut with more surface area for a better bond
  • A single interior adhesive liner for quicker application
  • New durable, low-profile lap seal with wider release tab, stays closed and looks neat
  • Easy to install – an excellent choice for retrofit Applications
  • 25/50 rated for use in air plenums
  • Fiber-free, formaldehyde-free, low VOC and nonparticulating formulation protects indoor air quality
  • Microban® antimicrobial product protection inhibits the growth of mold and mildew in the insulation

Information provided by Armacell®

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Water Absorption 0.20 %0.20 %3/8"- 1" Walls; ASTM C209
 0.20 %0.20 %1 1/2" and 2" Walls; ASTM C209
 
Thermal PropertiesMetricEnglishComments
Thermal Conductivity  0.0353 W/m-K
@Temperature 24.0 °C
0.245 BTU-in/hr-ft²-°F
@Temperature 75.2 °F
3/8"- 1" Walls; ASTM C177 or C518
 0.0366 W/m-K
@Temperature 32.0 °C
0.254 BTU-in/hr-ft²-°F
@Temperature 89.6 °F
3/8"- 1" Walls; ASTM C177 or C518
 0.0400 W/m-K
@Temperature 24.0 °C
0.278 BTU-in/hr-ft²-°F
@Temperature 75.2 °F
1 1/2" and 2" Walls; ASTM C177 or C518
 0.0410 W/m-K
@Temperature 32.0 °C
0.285 BTU-in/hr-ft²-°F
@Temperature 89.6 °F
1 1/2" and 2" Walls; ASTM C177 or C518
Maximum Service Temperature, Air 105 °C221 °F3/8"- 1" Walls; ASTM C534
 105 °C221 °F1 1/2" and 2" Walls; ASTM C534
Minimum Service Temperature, Air -183 °C-297 °F3/8"- 1" Walls; ASTM C534
 -183 °C-297 °F1 1/2" and 2" Walls; ASTM C534
Flame Spread Index 25253/8"- 1" Walls; ASTM E84
 25251 1/2" and 2" Walls; ASTM E84
 
Descriptive Properties
Bacterial ResistancePassed3/8"- 1" Walls, ASTM G22
 Passed1 1/2" and 2" Walls, ASTM G22
Fungi ResistancePassed3/8"- 1" Walls, ASTM G21/C1338
 Passed1 1/2" and 2" Walls, ASTM G21/C1338
Mold GrowthPassed3/8"- 1" Walls, UL181
 Passed1 1/2" and 2" Walls, UL181
Smoke Developed Index503/8"- 1" Walls, ASTM E84
 501 1/2" and 2" Walls, ASTM E84
Water Vapor Permeability0.05 perm-in3/8"- 1" Walls, ASTM E96, Procedure A
 0.08 perm-in1 1/2" and 2" Walls, ASTM E96, Procedure A

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Armacell ArmaSound® RD240 Sound Adsorption Insulation
Armacell AP Armaflex® White and Black Tube Insulation Through 1" Wall
Armacell AP Armaflex® FS 1 1/2" & 2" Duct Liner
Armacell AF/Armaflex® Insulation
Armacell AC/Accoflex® Tube Insulation

PARMD002 / 186613

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.