MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Covestro Baybond® PU 406 Polyurethane
Categories: Polymer; Thermoplastic; Polyurethane, TP

Material Notes: Baybond PU 406 is a non-ionic polyurethane polymer. It is used as the film-forming component in glass fiber sizes.

Properties / Applications: Baybond PU 406 was developed for the sizing of glass fibers used to reinforce thermoplastics. It has good film-forming properties and adhesion. Baybond PU 406 remains stable when exposed to shear forces. As with any product, use of Baybond PU 406 in a given application must be tested (including but not limited to field testing) in advance by the user to determine suitability.

Information provided by Covestro

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.10 g/cc0.0397 lb/in³
Volatiles 64 - 67 %64 - 67 %0.9-1.1g / 1h / 125°C, convection oven
pH 5.5 - 7.55.5 - 7.5
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 20.0 MPa2900 psi
Elongation at Break 700 %700 %
100% Modulus 3.70 MPa
@Strain 100 %
537 psi
@Strain 100 %
 
Thermal PropertiesMetricEnglishComments
Glass Transition Temp, Tg -72.0 °C-97.6 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Ensinger Hydex™ 202 Rigid Polyurethane (PU)
Covestro Baybond® PU 401 A Polyester Urethane Polymer
Ensinger Hydex™ 301 Rigid Polyurethane (PU)
Covestro Baybond® PU 402 A Polyester Urethane Polymer
Covestro Baybond® PU 330 Polyester Urethane Polymer

PCOVEST0073 / 201856

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.