MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ineos H12Z-02 Polypropylene Homopolymer, Antistatic and Nucleated
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene, Molded

Material Notes: A nucleated and antistated polypropylene homopolymer produced by Ineos utilizing unique catalyst technology. It is designed for injection molding applications that require superior mold release properties. This material meets the Food and Drug Administration requirements of 21CFR 177.1520.

Key Words: Nucleated and antistated
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.910 g/cc0.0329 lb/in³ASTM D792
Melt Flow 13 g/10 min
@Load 2.16 kg,
Temperature 230 °C
13 g/10 min
@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 100100ASTM D785
Hardness, Shore D 7171ASTM D2240
Tensile Strength at Break 17.4 MPa2520 psi2.0 in/min; ASTM D638
Tensile Strength, Yield 37.0 MPa5370 psi2.0 in/min; ASTM D638
Elongation at Break 75 %75 %2.0 in/min; ASTM D638
Elongation at Yield 9.0 %9.0 %2.0 in/min; ASTM D638
Flexural Modulus, 1% Secant 1830 MPa265000 psiASTM D790A
Izod Impact, Notched 0.427 J/cm0.800 ft-lb/inASTM D256
Izod Impact, Notched (ISO) 3.99 kJ/m²1.90 ft-lb/in²Area; ASTM D256
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 116 °C241 °FUnannealed; ASTM D648
 
Optical PropertiesMetricEnglishComments
Haze 56 %
@Thickness 1.27 mm
56 %
@Thickness 0.0500 in
ASTM D1003
Gloss 90 %90 %60°; ASTM D2457
 
Compliance PropertiesMetricEnglishComments
FDA YesYes
 
Descriptive Properties
ProcessInjection
 Injection Molding

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Ineos H12E-00 Polypropylene Homopolymer, Antistatic
Ineos H11G-01 Polypropylene Homopolymer
Ineos H28E-00 Polypropylene Homopolymer, Antistatic
Ineos R55C-00 Clarified Polypropylene Copolymer
Ineos H02C-00 Polypropylene Homopolymer

PSOLL4 / 68250

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.