Description: BR® 680-3 paste adhesive is a radar transparent, viscous/thixotropic material supplied at 60 – 65% solids. It is intended for bonding both metallic and non-metallic sandwich structures. It is equally suitable for bonding metals and composite laminates.BR 680-3 is co-curable at temperatures up to 700°F (371°C) with various polyimide composites. Although not mandatory, BR® 680 adhesive primer may be used to seal prepared metal surfaces. Features & Benefits: - 700°F (371°C) service temperature
- Developed specifically for honeycomb sandwich bonding
- 350°F (177°C) processing
- Radar transparent
- Superior thermal oxidative stability
- Co-curable with Avimid N and other poyimide composite materials
- Condensation-type polyimide
Applications: - Honeycomb sandwich construction
- Metal-to-metal bonding
- Composite-to-metal bonding
- Composite-to-composite bonding
Information provided by Cytec, subsequently acquired by Solvay. |