MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

DuPont Elvaloy® 1126 AC Ethylene and 25% Methyl Acrylate Copolymer  (discontinued **)
Categories: Polymer; Film; Thermoplastic; Ethylene Methyl Acrylate; Ethylene-Methyl Acrylate Copolymer, Molding Grade

Material Notes: Elvaloy® 1126 AC is intended for coextrusion and molding. It can be recommended for blow molding of parts requiring permanent flexibility, stress cracking resistance and softness. Excellent filler acceptance makes Elvaloy® 1126 AC suitable for highly filled compounds.

Elvaloy® 1126 AC is easily processed on standard equipment used for low-density polyethylene.

Information provided by DuPont.

This product line/trade name was acquired by Dow, but this specific grade was discontinued prior to the acquisition.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.944 g/cc0.0341 lb/in³ASTM D792 - ISO 1183
Melt Flow 0.60 g/10 min
@Load 2.16 kg,
Temperature 190 °C
0.60 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ASTM D1238 - ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 7878ASTM D2240 - ISO 868
Hardness, Shore D 1919ASTM D2240 - ISO 868
Tensile Strength at Break 14.0 MPa2030 psi500 mm/min; ASTM D638 - ISO 527-2
Elongation at Break 860 %860 %500 mm/min; ASTM D638 - ISO 527-2
Tensile Modulus 0.0190 GPa2.76 ksi1 mm/min; ASTM D638 - ISO 527-2
 
Thermal PropertiesMetricEnglishComments
Melting Point 90.0 °C194 °FBy DSC; ASTM D3418 - ISO 3146
Vicat Softening Point 45.0 °C113 °FA50 (10N); ASTM D1525 - ISO 306
 
Processing PropertiesMetricEnglishComments
Processing Temperature 140 - 160 °C284 - 320 °FFor blow molding
Rear Barrel Temperature 150 °C302 °FExtrusion lamination and extrusion coating
 150 °C302 °FCast film
 150 °C302 °FBlown film
Middle Barrel Temperature 160 °C320 °FBlown film
 210 °C410 °FCast film
 220 °C428 °FExtrusion lamination
Front Barrel Temperature 170 °C338 °FBlown film
 250 °C482 °FCast film
 290 °C554 °FExtrusion lamination
Adapter Temperature 180 °C356 °FBlown film
 250 °C482 °FCast Film
 290 °C554 °FExtrusion lamination
Die Temperature 180 °C356 °FBlown film
 250 °C482 °FCast film
 290 °C554 °FExtrusion lamination
 
Descriptive Properties
MA-Content25 wt.%DuPont Method

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Dow Nucrel® 0411HS Ethylene-Methacrylic Acid Copolymer Resin for Extrusion Coating/Laminating
Dow Elvaloy® 1125 AC Ethylene and 25% Methyl Acrylate Copolymer
Dow Elvaloy® 1820 AC Ethylene and 20% Methyl Acrylate Copolymer
Dow Elvaloy® 1224 AC Ethylene and 24% Methyl Acrylate Copolymer
Dow Elvaloy® 1218 AC Ethylene and 18% Methyl Acrylate Copolymer

PDUPM051 / 33718

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.