MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Lubrizol Estane® ZHF 90AT0 Thermoplastic Polyurethane, Flame Retardant
Categories: Polymer; Thermoplastic; Polyurethane, TP; Thermoplastic Polyurethane (TPUR), Polyether Grade

Material Notes: Type: Estane® ZHF 90AT0 TPU is a clear, glossy, zero halogen flame retardant polyether based thermoplastic polyurethane compound.

Features: Outstanding TPU properties.

Uses: Cable jacket and tube/hose and injection molding and fabric coating

Available in Americas, Europe, Middle East, Africa, India and Asia

Information Provided by The Lubrizol Corporation

Key Words: TPU
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.16 g/cc1.16 g/ccASTM D792
Maximum Moisture Content 0.0200.020
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 91
@Time 5.00 sec
91
@Time 0.00139 hour
ASTM D2240
Tensile Strength, Ultimate 46.5 MPa6750 psiASTM D412
Elongation at Break 400 %400 %ASTM D412
100% Modulus 10.0 MPa
@Strain 100 %
1450 psi
@Strain 100 %
ASTM D412
300% Modulus 29.0 MPa
@Strain 300 %
4210 psi
@Strain 300 %
ASTM D412
Tear Strength 25.2 kN/m144 pliTrouser; ASTM D470
Graves Tear Strength 102 kN/m583 pliDie C; ASTM D624
Taber Abrasion, mg/1000 Cycles 54
@Load 1.00 kg
54
@Load 2.20 lb
H-18 wheel; ASTM D3389
 
Thermal PropertiesMetricEnglishComments
Melting Point 172 °C342 °FDSC
Glass Transition Temp, Tg -38.0 °C-36.4 °FDSC
Flammability, UL94 V-2
@Thickness 0.762 mm
V-2
@Thickness 0.0300 in
Vertical Flame Test; ASTM D3801
 
Processing PropertiesMetricEnglishComments
Zone 1 180 °C356 °FExtrusion
Zone 2 185 °C365 °FExtrusion
Zone 3 190 °C374 °FExtrusion
Zone 4 195 °C383 °FExtrusion
Adapter Temperature 195 °C383 °F5, Extrusion
Die Temperature 205 °C401 °FZone 2, Extrusion
 205 °C401 °F6, Zone 1, Extrusion
Drying Temperature 180 °C356 °F
Dry Time 2.00 - 4.00 hour2.00 - 4.00 hour
Dew Point -40.0 °C-40.0 °F
 
Descriptive Properties
RT Burst Pressure4.3 MPaISO 7628/1

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Lubrizol ESTANE® 58244 Ether Based Thermoplastic Polyurethane
Lubrizol Estane® ZHF90AT2 NAT 055 Thermoplastic Polyurethane
Lubrizol Estane® ZHF 95AT3 Thermoplastic Polyurethane, Flame Retardant
BASF Elastollan® SP 806 TPUR
Taiwan PU Corporation TPU-BH90 Hydrolysis Resistance, Blow Molding Polyether Base TPU

PNOVEON599 / 121490

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.