MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Zinc ZA-8 (Zn-8Al-1Cu-0.02Mg), Permanent Mold Cast
Categories: Metal; Nonferrous Metal; Zinc Alloy

Material Notes: Recommended Casting Temperature 435-460°C

Key Words: ASTM B791; ASTN B669; UNS Z35635 (Ingot); UNS Z35636 (castings)
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 6.30 g/cc0.228 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Brinell 8787500 kg load; 10 mm hardened steel ball
Hardness, Knoop 111111Estimated from Brinell Value
Hardness, Rockwell A 3737Estimated from Brinell Value
Hardness, Rockwell B 5454Estimated from Brinell Value
Hardness, Vickers 100100Estimated from Brinell Value
Tensile Strength, Ultimate 240 MPa
@Diameter 12.7 mm
34800 psi
@Diameter 0.500 in
Tensile Strength, Yield 208 MPa
@Strain 0.2 %
30200 psi
@Strain 0.2 %
Elongation at Break 1.3 %1.3 %in 5 cm
Modulus of Elasticity 85.5 GPa12400 ksi
Compressive Strength 210 MPa30500 psi
Fatigue Strength 52.0 MPa
@# of Cycles 5.00e+8
7540 psi
@# of Cycles 5.00e+8
Reverse Bend
Shear Strength 242 MPa35100 psi
Charpy Impact, Unnotched 20.0 J
@Thickness 10.0 mm
14.8 ft-lb
@Thickness 0.394 in
square bar
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.00000620 ohm-cm0.00000620 ohm-cm
 
Thermal PropertiesMetricEnglishComments
Heat of Fusion 112 J/g48.2 BTU/lb
CTE, linear 23.2 µm/m-°C
@Temperature 20.0 °C
12.9 µin/in-°F
@Temperature 68.0 °F
Specific Heat Capacity 0.435 J/g-°C0.104 BTU/lb-°F
Thermal Conductivity 115 W/m-K798 BTU-in/hr-ft²-°F
Melting Point 375 - 404 °C707 - 759 °F
Solidus 375 °C707 °F
Liquidus 404 °C759 °F
 
Processing PropertiesMetricEnglishComments
Casting Temperature 435 - 460 °C815 - 860 °F
 
Component Elements PropertiesMetricEnglishComments
Aluminum, Al 8.0 - 8.8 %8.0 - 8.8 %Addition, Casting
 8.2 - 8.8 %8.2 - 8.8 %Addition, Ingot form
Cadmium, Cd <= 0.0050 %<= 0.0050 %Impurity, Ingot form
 <= 0.0060 %<= 0.0060 %Impurity, Casting
Copper, Cu 0.80 - 1.3 %0.80 - 1.3 %Addition, Casting
 0.80 - 1.3 %0.80 - 1.3 %Addition, Ingot form
Iron, Fe <= 0.065 %<= 0.065 %Impurity, Ingot form
 <= 0.075 %<= 0.075 %Impurity, Casting
Lead, Pb <= 0.0050 %<= 0.0050 %Impurity, Ingot form
 <= 0.0060 %<= 0.0060 %Impurity, Casting
Magnesium, Mg 0.015 - 0.030 %0.015 - 0.030 %Addition, Casting
 0.020 - 0.030 %0.020 - 0.030 %Addition, Ingot form
Tin, Sn <= 0.0020 %<= 0.0020 %Impurity, Ingot form
 <= 0.0030 %<= 0.0030 %Impurity, Casting
Zinc, Zn 89.793 - 90.98 %89.793 - 90.98 %As balance; Ingot per ASTM B 669
 89.78 - 91.185 %89.78 - 91.185 %As balance; Castings per ASTM B 791

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Zinc ZA-8 (Zn-8Al-1Cu-0.02Mg), Die Cast
Zinc ZA-27 (Zn-27Al-2Cu-0.015Mg), Die Cast
Zinc ZA-12 (Zn-11Al-1Cu-0.025Mg), Die Cast
Zinc AC41A Alloy (Zamak 5), As Cast
Copper-Hardened Rolled Zinc (Zn-1.0Cu), Cold-Rolled

MZN801 / 14567

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.