MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Polyram RamSter PF353M6 PBT, 30% Mineral Filled
Categories: Polymer; Thermoplastic; Polyester, TP; Polybutylene Terephthalate (PBT); Polybutylene Terephthalate (PBT), Mineral Filled

Material Notes: 30% mineral filled for injection molding applications

Information provided by Polyram Ram On Ind.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.45 g/cc0.0524 lb/in³DIN 53479
Water Absorption 0.50 %0.50 %DIN 53495
Moisture Absorption at Equilibrium 0.20 %0.20 %23° C, 50% RH; DIN 53714
Linear Mold Shrinkage 0.018 cm/cm0.018 in/in
Melt Flow 15 g/10 min
@Load 2.16 kg,
Temperature 250 °C
15 g/10 min
@Load 4.76 lb,
Temperature 482 °F
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 58.0 MPa8410 psiASTM-D638
Elongation at Break 4.0 %4.0 %ASTM-D638
Flexural Strength 110 MPa16000 psiASTM D790
Flexural Modulus 4.50 GPa653 ksiASTM-D790
Izod Impact, Notched 0.450 J/cm
@Temperature 23.0 °C
0.843 ft-lb/in
@Temperature 73.4 °F
ASTM-D256
 
Electrical PropertiesMetricEnglishComments
Dielectric Constant 3.6
@Frequency 1e+6 Hz
3.6
@Frequency 1e+6 Hz
VDE 0303/4
 
Thermal PropertiesMetricEnglishComments
Melting Point 225 °C437 °F
Deflection Temperature at 0.46 MPa (66 psi) 160 °C320 °FDIN 53461
Deflection Temperature at 1.8 MPa (264 psi) 70.0 °C158 °FDIN 53461
Flammability, UL94 HB
@Thickness 3.00 mm
HB
@Thickness 0.118 in
Glow Wire Test 650 °C1200 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Overview of materials for Polybutylene Terephthalate (PBT), Mineral Filled
A. Schulman ComAlloy Hiloy® 419 Polyester - PBT, Mineral Reinforced
LG Chemical Lupox® SG3180S PBT+PET+MF18%
Evonik Vestodur® RS 1409 30% Mineral Reinforced, Radiation Crosslinkable PBT
Overview of materials for Polybutylene Terephthalate (PBT), 30% Glass Fiber Filled

PPOLYRA152 / 57414

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.