MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

INEOS Styrolution Styrolux® GH 58 SBC
Categories: Polymer; Thermoplastic; Styrene-Butadiene; Styrene-Butadiene Copolymer, SBC

Material Notes: Description: Styrolux® GH 58 is a high flow thermoplastic styrene-butadiene block copolymer with excellent mold release properties. It has crystal clarity, good toughness, good stiffness and warpage resistance for general molding applications. Styroclear GH 58 may be suitable for conventional thermoplastics processing technologies such as injection molding.

Information provided by STYROLUTION, which is a joint venture between BASF and INEOS

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Melt Flow 16 g/10 min16 g/10 minASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 7474ASTM D2240
Tensile Strength, Yield 28.0 MPa4060 psi2in/min; ASTM D638
Elongation at Break 43 %43 %ASTM D638
Tensile Modulus 1.68 GPa244 ksi2in/min; ASTM D882
Flexural Strength 33.0 MPa4790 psiASTM D790
Flexural Modulus 1.50 GPa218 ksiASTM D790
Dart Drop, Total Energy 0.600 J0.443 ft-lbTotal energy; ASTM D3763
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 1.8 MPa (264 psi) 67.0 °C153 °FASTM D648
Vicat Softening Point 90.0 °C
@Load 1.02 kg
194 °F
@Load 2.25 lb
Rate 120°C/hr; ASTM D1525
 
Optical PropertiesMetricEnglishComments
Transmission, Visible 90 %90 %ASTM D1003
 
Processing PropertiesMetricEnglishComments
Melt Temperature 180 - 235 °C356 - 455 °FInjection
Mold Temperature 30.0 - 50.0 °C86.0 - 122 °F
 
Descriptive Properties
Commercial StatusNorth America

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Chi Mei Kibiton® PB-5903 SBC
INEOS Styrolution Styrolux® 693D SBC
Chi Mei Kibiton® PB-5502 Styrene-Butadiene Copolymer
INEOS Styrolution Styrolux® S SBC
Nitriflex SB-1006 A Styrene Butadiene Copolymer

PBASG0636 / 132269

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.