MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

KEP Kepital® FG2025 25% Glass Fiber Reinforced Acetal Copolymer
Categories: Polymer; Thermoplastic; Acetal (Polyoxymethylene, POM); Acetal Copolymer, 30% Glass Fiber Reinforced

Material Notes: Information provided by US distributor Polymer Technology and Services, LLC (PTS).

Key Words: Polyacetal; Polyoxymethylene; Korea Engineering Plastics
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.59 g/cc0.0574 lb/in³ASTM D792
Water Absorption 0.20 %0.20 %24 hours at 73°F
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell M 9595ASTM D785
Tensile Strength, Yield 136.8 MPa
@Thickness 3.17 mm
19840 psi
@Thickness 0.125 in
Elongation at Break 3.0 %
@Thickness 3.17 mm
3.0 %
@Thickness 0.125 in
Flexural Yield Strength 205.2 MPa
@Thickness 3.17 mm
29760 psi
@Thickness 0.125 in
Flexural Modulus 9.03 GPa
@Thickness 3.17 mm
1310 ksi
@Thickness 0.125 in
Izod Impact, Notched 0.960 J/cm
@Thickness 3.17 mm
1.80 ft-lb/in
@Thickness 0.125 in
 
Thermal PropertiesMetricEnglishComments
Melting Point 203 °C397 °FASTM D789
Deflection Temperature at 0.46 MPa (66 psi) 164 °C327 °FASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 163 °C325 °FASTM D648
Flammability, UL94 HB
@Thickness 1.59 mm
HB
@Thickness 0.0625 in
 
Processing PropertiesMetricEnglishComments
Rear Barrel Temperature 165 - 180 °C329 - 356 °F
Middle Barrel Temperature 175 - 195 °C347 - 383 °F
Front Barrel Temperature 180 - 195 °C356 - 383 °F
Nozzle Temperature 180 - 195 °C356 - 383 °F
Melt Temperature 185 - 220 °C365 - 428 °F
Mold Temperature 70.0 - 90.0 °C158 - 194 °F
Drying Temperature 80.0 - 90.0 °C176 - 194 °F
Dry Time 3 - 4 hour3 - 4 hour
Injection Pressure 48.3 - 117 MPa7000 - 17000 psi

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
KEP Kepital® FG2025K Acetal Copolymer, 10% Glass Fiber
304 Stainless Steel
KEP Kepital® FG2025 Acetal Copolymer, 25% Glass Fiber
Samyang Trirex® PC-3022IR 15 MFI Clear Polycarbonate With Release
Lotte Advanced Materials Starex® SD-0150 ABS, Unreinforced

PLBK02 / 50372

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.