LATI Latilub 88/10-15T K/30 PEEK, 30% Carbon Fiber Reinforced, PTFE Filled
Categories:
Polymer
;
Thermoplastic
;
Polyketone
;
Polyetheretherketone (PEEK)
;
Polyetheretherketone, PEEK, Carbon Fiber Filled
Material Notes:
Self-lubricating product based on Polyetheretherketone (PEEK). PTFE. Carbon fiber.
Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North America
Information provided by Lati Industria Termoplastici S.p.A.
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Metric
English
Comments
Density
1.47
g/cc
0.0531
lb/in³
Linear Mold Shrinkage, Flow
0.0010
-
0.0030
cm/cm
0.0010
-
0.0030
in/in
Linear Mold Shrinkage, Transverse
0.0035
-
0.0055
cm/cm
0.0035
-
0.0055
in/in
Mechanical Properties
Metric
English
Comments
Tensile Strength at Break
170
MPa
24700
psi
Elongation at Break
1.0 %
1.0 %
Tensile Modulus
22.7
GPa
3290
ksi
Charpy Impact Unnotched
2.70
J/cm²
12.8
ft-lb/in²
Charpy Impact, Notched
0.500
J/cm²
2.38
ft-lb/in²
Coefficient of Friction, Dynamic
0.24
0.24
Coefficient of Friction, Static
0.30
0.30
K (wear) Factor
6.00
x 10
-8
mm³/N-M
2.98
x 10
-10
in³-min/ft-lb-hr
Thermal Properties
Metric
English
Comments
Deflection Temperature at 0.46 MPa (66 psi)
350
°C
662
°F
Deflection Temperature at 1.8 MPa (264 psi)
350
°C
662
°F
Vicat Softening Point
350
°C
@Load 5.00 kg
662
°F
@Load 11.0 lb
Processing Properties
Metric
English
Comments
Melt Temperature
370
-
400
°C
698
-
752
°F
Mold Temperature
170
-
200
°C
338
-
392
°F
Drying Temperature
120
-
150
°C
@Time 10800 sec
248
-
302
°F
@Time 3.00 hour
Descriptive Properties
ISO Shrinkage - Pressure
60 MPa
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to view all the property values for this datasheet as they were originally entered into MatWeb.
Users viewing this material also viewed the following:
Ensinger Tecapeek® XP-99 Compression Molded PEEK Compound, Bearing Grade Material with 7% Graphite, 8% PTFE, and 15% Carbon Fiber
Greene Tweed Arlon® 1555 PEEK, Carbon, Graphite Filled
LATI Latilub 88/50-20GRT K/10 PEEK, 10% Carbon Fiber Reinforced, Graphite/PTFE Filled
Hippe PEEK BG Polyetheretherketone with carbon fiber, PTFE and graphite
LATI Latilub 88/10-15T G/30 PEEK, 30% Glass Fiber Reinforced, PTFE Filled
PLATH9906 / 177602
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
webmaster@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.