MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Hexcel® HexForce™ 383 Aramid Fabric  (discontinued **)
Categories: Other Engineering Material; Composite Fibers; Polymer; Thermoset; Aramid

Material Notes: Hexcel manufactures aramid fabrics for use in aerospace applications as well as marine, tooling and recreational products where high strength, low weight, and impact resistance are essential. Aramids display excellent dimensional stability with a slightly negative coefficient of thermal expansion (-2.4 X 10-6/ºC.) They are resistant to chemicals with the exception of a few strong acids and alkalis.
Aramids have excellent stability over a wide range of temperatures for prolonged periods. They show essentially no embrittlement or strength loss at temperatures as low as -320ºF (-196ºC). Aramids do not melt or support combustion but will start to carbonize at approximately 800ºF (427ºC).

Information provided by Hexcel

Key Words: Kevlar
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Thickness 330 microns13.0 mil
Fiber Count 2400 dtex2160 denierWarp yarn; Kevlar® 49
 2400 dtex2160 denierFill yarn; Kevlar® 49
 
Mechanical PropertiesMetricEnglishComments
Tensile Impact 55.5 J/cm104 ft-lb/inWarp
 55.5 J/cm104 ft-lb/inFilling
 
Thermal PropertiesMetricEnglishComments
CTE, linear -2.40 µm/m-°C-1.33 µin/in-°F
Maximum Service Temperature, Air 427 °C801 °Fstarts to carbonize
Minimum Service Temperature, Air -196 °C-321 °F
 
Descriptive Properties
Fabric Weight (oz/yd2)9.4Dry
Nominal Construction (count/in)16Warp
 16Fill
Weave Style5 Harness Satin

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Solvay Polyifilm Polyimide Vacuum Bagging Film
Solvay EF2000 Organosilicate Polymer
Solvay Vac-Pak® UHT750 Vacuum bagging film
Solvay 70000 Aramid Peel
Resinlab® RC8020 Anaerobic Retaining Compound

PHEXC493 / 101112

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.