DOW HDPE 38152M resin is a medium molecular weight distribution copolymer designed to offer good impact strength and stress crack resistance with excellent toughness. This resin has excellent processability over a wide range of molding conditions. Typical applications are base cups and general purpose applications. This material complies with FDA regulation 21 CFR 177.1520 (c) 3.1 for food contact applications. Data provided by Dow Chemical. |