MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Ti30Ta ß titanium alloy
Categories: Metal; Nonferrous Metal; Titanium Alloy; Beta Titanium Alloy

Key Words: medical, surgical
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Ultimate 740 MPa107000 psias rolled
 800 MPa116000 psiannealed at 1100°C
 800 MPa116000 psiannealed at 1400°C
Tensile Strength, Yield 590 MPa85600 psias rolled
 650 MPa94300 psi0.2%, annealed at 1100°C
 680 MPa98600 psi0.2%, annealed at 1400°C
Elongation at Break 6.0 %6.0 %annealed at 1400°C
 8.0 %8.0 %annealed at 1100°C
 28 %28 %as rolled
Reduction of Area 18 %18 %annealed at 1400°C
 42 %42 %annealed at 1100°C
 58 %58 %as rolled
Modulus of Elasticity 63.0 GPa9140 ksi1h / 1000°C / water
 80.0 GPa11600 ksiAs rolled
 
Component Elements PropertiesMetricEnglishComments
Tantalum, Ta 30 %30 %
Titanium, Ti 70 %70 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Ti30Nb ß titanium alloy
Ti12Mo5Zr5Sn ß titanium alloy
Ti15Mo5Zr3Al ß titanium alloy
Overview of materials for Silicone Rubber
Titanium Alloys, General

MMEDIC29 / 12405

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.