MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Röhm ACRYLITE® MD™ H12 Acrylic Polymer For Medical Diagnostics  (discontinued **)
Categories: Polymer; Thermoplastic; Acrylic (PMMA); Acrylic, Optical Grade, Molded; Acrylic, UV Stabilized, Molded

Material Notes: ACRYLITE® MD™ H12 acrylic polymer is an amorphous thermoplastic molding compound based on polymethyl methacrylate (PMMA) for the medical diagnostic industry.

Typical properties of ACRYLITE® MD™ acrylic polymers are exceptional ultra-violet light transmittance (UVT), exceptional optical clarity, and good dimensional stability for controlled fluid flow.

The special properties of ACRYLITE MD™ L40 polymer are medium heat resistance, medium melt flow rate, UV light transmitting, and lubricant free.

Application: Used for injection molded thin-wall medical devices requiring UV spectroscopy for fluid evaluation.

Information Provided by Evonik CYRO. The former Evonik Methacrylates business has been sold to Röhm (Roehm) GmbH.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.19 g/cc1.19 g/ccASTM D792
Bulk Density 0.660 g/cc0.0238 lb/in³ASTM D1895
Water Absorption at Saturation 0.30 %0.30 %ASTM D570
Linear Mold Shrinkage 0.0040 - 0.0060 cm/cm0.0040 - 0.0060 in/inASTM D955
Melt Flow 7.0 g/10 min
@Load 3.80 kg,
Temperature 230 °C
7.0 g/10 min
@Load 8.38 lb,
Temperature 446 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell M 9494ASTM D785
Tensile Strength at Break 65.5 MPa9500 psiASTM D638
Elongation at Break 4.0 - 6.0 %4.0 - 6.0 %ASTM D638
Elongation at Yield 4.0 - 6.0 %4.0 - 6.0 %ASTM D638
Tensile Modulus 3.24 GPa470 ksiASTM D638
Flexural Strength 117 MPa17000 psiASTM D790
Flexural Modulus 3.38 GPa490 ksiASTM D790
Izod Impact, Notched 0.192 J/cm
@Temperature 23.0 °C
0.360 ft-lb/in
@Temperature 73.4 °F
1/4" bar; ASTM D256
 
Thermal PropertiesMetricEnglishComments
CTE, linear 72.0 µm/m-°C
@Temperature 0.000 - 156 °C
40.0 µin/in-°F
@Temperature 32.0 - 312 °F
ASTM D696
Deflection Temperature at 1.8 MPa (264 psi) 93.9 °C
@Thickness 6.35 mm
201 °F
@Thickness 0.250 in
Annealed; ASTM D648
Vicat Softening Point 105 °C221 °FASTM D1525
 
Optical PropertiesMetricEnglishComments
Haze <= 1.0 %<= 1.0 %ASTM D1003
Yellow Index <= 1.0 %<= 1.0 %ASTM D1925
Transmission, Visible 92 %92 %ASTM D1003
UV Transmittance >= 87.7 %>= 87.7 %340 nm
 
Processing PropertiesMetricEnglishComments
Middle Barrel Temperature 221 - 249 °C430 - 480 °F
Melt Temperature 221 - 249 °C430 - 480 °F
Mold Temperature 32.2 - 79.4 °C90.0 - 175 °F
Drying Temperature 76.7 °C170 °F
Dry Time 3 - 4 hour3 - 4 hour

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Röhm ACRYLITE® MD™ L40 Acrylic Polymer For Medical Diagnostics
Röhm Acrylite® 8N Acrylic Polymer
Plaskolite West Optix® CA - 51 HF UVT General Purpose Acrylic Resin
Röhm Acrylite Plus® zdf Impact Acrylic Polymer
Röhm Acrylite Plus® zk3HR Impact Acrylic Polymer

PCYR00053 / 101042

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.