Property
|
Metals
|
Trade Name
|
Manufacturer
|
Recently Viewed Materials
NOVA Chemicals Novapol® TR-0735-UG Hexene MDPE Rotational Molding Resin
Categories:
Polymer
;
Thermoplastic
;
Polyethylene (PE)
;
Medium Density (MDPE)
;
Medium Density Polyethylene (MDPE), Rotational Molded
Material Notes:
Features:
Good impact properties
Excellent processability
NSF listed for Stds. 14, 24 and 61
Applications:
Toys
Complex custom parts
Home and garden items
Mailboxes
Information provided by Nova Chemicals
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Metric
English
Comments
Density
0.935
g/cc
0.0338
lb/in³
ASTM D792
ESCR 100% Igepal®
>=
1000
hour
>=
1000
hour
Condition A; ASTM D1693
ESCR 10% Igepal®
220
hour
220
hour
Condition A; ASTM D1693
Melt Flow
7.0
g/10 min
@Load 2.16 kg,
Temperature 190 °C
7.0
g/10 min
@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Mechanical Properties
Metric
English
Comments
Tensile Strength, Yield
17.3
MPa
2510
psi
ASTM D638
Flexural Modulus
0.780
GPa
113
ksi
ASTM D790
Impact Test
67.8
J
@Thickness 3.17 mm
50.0
ft-lb
@Thickness 0.125 in
ARM Method
203
J
@Thickness 6.35 mm
150
ft-lb
@Thickness 0.250 in
ARM Method
Thermal Properties
Metric
English
Comments
Deflection Temperature at 0.46 MPa (66 psi)
47.0
°C
117
°F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi)
37.3
°C
99.1
°F
ASTM D648
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to view all the property values for this datasheet as they were originally entered into MatWeb.
Users viewing this material also viewed the following:
NOVA Chemicals NOVAPOL® TR-0735-U LLDPE Rotational Molding Resin
NOVA Chemicals Novapol® TR-0735-U Hexene MDPE Rotational Molding Resin
PNOV917 / 54863
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
webmaster@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.