MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Chemically Resistant adhesives

Cotronics Duralco™ 4460 Electrically Resistant, Low Viscosity Epoxy Adhesive, Coating, and Sealant
Categories: Polymer; Thermoset; Epoxy

Material Notes: Excellent adhesion to metals, plastics, ceramics and glass. High bond strength, low moisture absorption, high thermal stability, low shrinkage and excellent chemical, electrical, and radiation resistance.

Applications: Ideal for ultra thin bond lines, sealing porous materials and protecting boding and coating critical electronic components, strain gauges, etc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.10 g/cc0.0397 lb/in³
Moisture Absorption at Equilibrium 0.10 %0.10 %
Viscosity 600 cP600 cP
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 8080
Tensile Strength, Ultimate 71.0 MPa10300 psi
Elongation at Break 5.0 %5.0 %
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+14 ohm-cm1.00e+14 ohm-cm
Dielectric Strength 19.7 kV/mm500 kV/in
 
Thermal PropertiesMetricEnglishComments
CTE, linear 64.0 µm/m-°C
@Temperature 20.0 °C
35.6 µin/in-°F
@Temperature 68.0 °F
Thermal Conductivity 0.576 W/m-K4.00 BTU-in/hr-ft²-°F
Maximum Service Temperature, Air 316 °C600 °F
Shrinkage 0.50 %0.50 %
 
Processing PropertiesMetricEnglishComments
Cure Time 240 min
@Temperature 121 °C
4.00 hour
@Temperature 250 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Cotronics Duralco™ 4461 Electrically Resistant, Low Viscosity Epoxy Adhesive, Coating, and Sealant
Cotronics Duralco™ 128 500°F (260°C) Ceramic Filled Epoxy
Epoxy Technology EPO-TEK® H61 Thermally Conductive Epoxy
Epoxy Technology EPO-TEK® T905-1 Thermally Conductive, Electrically Insulating Epoxy
Epoxy Technology EPO-TEK® H70E-TI Thermally Conductive, Electrically Insulating Epoxy

PCOTR0410 / 29066

Chemically Resistant adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.