MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Arkema Kynar® 720E PVDF
Material Notes:

Information provided by Arkema.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Water Absorption 0.020 %0.020 %Dry; Sim. to ISO 62
Linear Mold Shrinkage, Flow 0.020 cm/cm0.020 in/inDry; ISO 294-4, 2577
 0.020 cm/cm0.020 in/in
Melt Flow 14.8 g/10 min
@Load 3.80 kg,
Temperature 230 °C
14.8 g/10 min
@Load 8.38 lb,
Temperature 446 °F
cm³/10 min Volumetric Rate; ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 54.0 MPa7830 psiDry; ISO 527-1/-2
Elongation at Break >= 50 %>= 50 %Dry; ISO 527-1/-2
Elongation at Yield 8.0 %8.0 %Dry; ISO 527-1/-2
Tensile Modulus 2.20 GPa319 ksiDry; ISO 527-1/-2
Charpy Impact, Notched 0.800 J/cm²
@Temperature 23.0 °C
3.81 ft-lb/in²
@Temperature 73.4 °F
Dry; ISO 179/1eA
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 150 µm/m-°C83.3 µin/in-°FDry; ISO 11359-1/-2
Thermal Conductivity 0.190 W/m-K
@Temperature 230 °C
1.32 BTU-in/hr-ft²-°F
@Temperature 446 °F
Melt
Melting Point 169 °C336 °F10°C/min; Dry; ISO 11357-1/-3
Deflection Temperature at 1.8 MPa (264 psi) 104 °C219 °FDry; ISO 75-1/-2
Glass Transition Temp, Tg -40.0 °C-40.0 °F10°C/min; Dry; ISO 11357-1/-2
Flammability, UL94 V-0V-0Yellow Card Available; Dry; IEC 60695-11-10
Oxygen Index 66 %66 %Dry; ISO 4589-1/-2
 
Processing PropertiesMetricEnglishComments
Processing Temperature 230 °C446 °FCompression Molding; Molding Temperature; ISO 293
Melt Temperature 190 - 270 °C374 - 518 °F
 230 °C446 °FInjection Molding; ISO 294
Mold Temperature 23.0 - 90.0 °C73.4 - 194 °F
 90.0 °C194 °FInjection Molding; ISO 10724
 
Descriptive Properties
Compression Molding Demolding Temperature (°C)40ISO 293
Form as DeliveredPellets
Moisture SensitiveNo
Processing MethodsFilm Extrusion
 Injection Molding

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Arkema KYNAR® 460 Polyvinylidene Fluoride Homopolymer - Extrusion
Arkema KYNAR FLEX® 2800-00 Polyvinylidene Fluoride Copolymer - Extrusion
Arkema KYNAR FLEX® 2800-20 Polyvinylidene Fluoride Copolymer - Extrusion & Molding
Arkema Kynar Superflex® 2500-20 PVDF
Arkema Kynar® 740E PVDF

PARKF735 / 193531

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.